<?xml version="1.0" encoding="UTF-8"?>
<mdt ver="2006" requires="2006" Ratio1Name="Si:Al" Ratio2Name="SiB:Al" OxideProperty1="Expan" RecipeProperty1="Cost/kg">
<oxides>
<oxide name="BaO" weight="153.30" property1="0.129" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="CaO" weight="56.10" property1="0.148" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="Li2O" weight="29.80" property1="0.068" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="MgO" weight="40.30" property1="0.026" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="K2O" weight="94.20" property1="0.331" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="Na2O" weight="62.00" property1="0.387" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="ZnO" weight="81.40" property1="0.094" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="SrO" weight="103.60" property1="0.130" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="F" weight="19.00" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="P2O5" weight="141.90" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="PbO" weight="223.20" property1="0.083" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="TiO2" weight="79.90" property1="0.144" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="Al2O3" weight="102.00" property1="0.063" unity1="no" unity2="yes" UnityIfReduction1="no" UnityIfReduction2="yes" UnityIfOxidation1="no" UnityIfOxidation2="yes" Ratio1="B" Ratio2="B"/>
<oxide name="B2O3" weight="69.60" property1="0.031" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="T"/>
<oxide name="SiO2" weight="60.10" property1="0.035" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="T" Ratio2="T"/>
<oxide name="CoO" weight="74.92" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="Cr2O3" weight="152.00" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="Cu2O" weight="143.00" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="CuO" weight="79.54" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="Fe2O3" weight="160.00" property1="0.125" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="FeO" weight="81.80" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="MnO" weight="70.90" property1="0.050" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="MnO2" weight="86.90" property1="0.050" unity1="yes" unity2="no" UnityIfReduction1="yes" UnityIfReduction2="no" UnityIfOxidation1="yes" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="NiO" weight="74.70" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="V2O5" weight="181.90" property1="0.000" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="SnO2" weight="150.71" property1="0.020" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="ZrO" weight="107.20" property1="0.020" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
<oxide name="ZrO2" weight="123.22" property1="0.020" unity1="yes" unity2="no" UnityIfReduction1="no" UnityIfReduction2="no" UnityIfOxidation1="no" UnityIfOxidation2="no" Ratio1="N" Ratio2="N"/>
</oxides>
<materials>
<types>
<type number="1" name="Abrasive Resistant Super Hard Material"/>
<type number="2" name="Additive"/>
<type number="3" name="Aggregate"/>
<type number="4" name="Alumina"/>
<type number="5" name="Aluminum Silicate"/>
<type number="6" name="Available from Laguna Clays"/>
<type number="7" name="Ball Clay"/>
<type number="8" name="Ceramic body and glaze binders, plasticizers"/>
<type number="9" name="Clay Other"/>
<type number="10" name="Colorant"/>
<type number="11" name="Electrolyte"/>
<type number="12" name="Eutectic"/>
<type number="13" name="Feldspar"/>
<type number="14" name="Fireclay"/>
<type number="15" name="Flux Source"/>
<type number="16" name="Frit"/>
<type number="17" name="Generic Material"/>
<type number="18" name="Kaolin"/>
<type number="19" name="Leaded Frit"/>
<type number="20" name="Low Expansion Material"/>
<type number="21" name="Materials used in Denmark"/>
<type number="22" name="Non-Oxide Material"/>
<type number="23" name="Opacifier"/>
<type number="24" name="Refractory"/>
<type number="25" name="Silica/Quartz"/>
<type number="26" name="Stoneware Clay"/>
</types>
<material name="A-3 Feldspar" weight="660.63181565613" dfnumber="24" searchkey="A3 Feldspar, Kona A-3 Feldspar, Kona A3 Feldspar" type="13" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.426214" analysis="4.000"/>
<oxide symbol="Al2O3" formula="1.055716" analysis="16.300"/>
<oxide symbol="SiO2" formula="7.873720" analysis="71.630"/>
<oxide symbol="Fe2O3" formula="0.002890" analysis="0.070"/>
<oxide symbol="CaO" formula="0.047104" analysis="0.400"/>
<oxide symbol="K2O" formula="0.526682" analysis="7.510"/>
</chemistry>
</material>
<material name="ABC Colemanite" weight="86.325387027883" dfnumber="2139" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.528371" analysis="42.600"/>
<oxide symbol="CaO" formula="0.455478" analysis="29.600"/>
<oxide symbol="SiO2" formula="0.008618" analysis="0.600"/>
<oxide symbol="MgO" formula="0.006426" analysis="0.300"/>
<oxide symbol="Fe2O3" formula="0.000540" analysis="0.100"/>
<oxide symbol="Na2O" formula="0.001392" analysis="0.100"/>
<oxide symbol="SrO" formula="0.008333" analysis="1.000"/>
<oxide symbol="Al2O3" formula="0.001693" analysis="0.200"/>
</chemistry>
</material>
<material name="Ajax P Kaolin" weight="265.47074622532" dfnumber="28" searchkey="Ajax P Casting Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.012853" analysis="0.300"/>
<oxide symbol="MgO" formula="0.019774" analysis="0.300"/>
<oxide symbol="TiO2" formula="0.046543" analysis="1.400"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.400"/>
<oxide symbol="SiO2" formula="2.002132" analysis="45.300"/>
<oxide symbol="CaO" formula="0.002367" analysis="0.050"/>
<oxide symbol="Fe2O3" formula="0.004980" analysis="0.300"/>
</chemistry>
</material>
<material name="Albany Slip" weight="459.33031085199" dfnumber="31" searchkey="New York Slip, Albany Clay" type="9" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.658897" analysis="14.630"/>
<oxide symbol="CaO" formula="0.475758" analysis="5.810"/>
<oxide symbol="SiO2" formula="4.419536" analysis="57.820"/>
<oxide symbol="K2O" formula="0.156053" analysis="3.200"/>
<oxide symbol="Fe2O3" formula="0.149586" analysis="5.210"/>
<oxide symbol="MgO" formula="0.308914" analysis="2.710"/>
<oxide symbol="Na2O" formula="0.059275" analysis="0.800"/>
<oxide symbol="TiO2" formula="0.022998" analysis="0.400"/>
</chemistry>
</material>
<material name="Alberta Slip" weight="356.61605815151" dfnumber="32" searchkey="Archie Bray Slip" type="9" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.128898" analysis="2.200"/>
<oxide symbol="Fe2O3" formula="0.102166" analysis="4.500"/>
<oxide symbol="MgO" formula="0.351539" analysis="3.900"/>
<oxide symbol="TiO2" formula="0.013639" analysis="0.300"/>
<oxide symbol="Al2O3" formula="0.541324" analysis="15.200"/>
<oxide symbol="K2O" formula="0.134968" analysis="3.500"/>
<oxide symbol="P2O5" formula="0.002560" analysis="0.100"/>
<oxide symbol="CaO" formula="0.382035" analysis="5.900"/>
<oxide symbol="SiO2" formula="3.236071" analysis="53.540"/>
</chemistry>
</material>
<material name="Alkatrol" weight="486.21245421245" dfnumber="38" searchkey="" type="5" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.067031" analysis="1.300"/>
<oxide symbol="Na2O" formula="0.101843" analysis="1.300"/>
<oxide symbol="TiO2" formula="0.030395" analysis="0.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="21.000"/>
<oxide symbol="SiO2" formula="5.907773" analysis="73.100"/>
<oxide symbol="Fe2O3" formula="0.012143" analysis="0.400"/>
</chemistry>
</material>
<material name="Alumina Hydrate" weight="155.98715399908" dfnumber="42" searchkey="Alum Hydrate, Alumina Trihydrate, Hydrated Alumina, Alpha Aluminum Trihydroxide, Gibbsite" type="4,17" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="65.390"/>
</chemistry>
</material>
<material name="Amtalc-C98" weight="124.95133682452" dfnumber="3088" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.078222" analysis="3.500"/>
<oxide symbol="TiO2" formula="0.001569" analysis="0.100"/>
<oxide symbol="K2O" formula="0.003993" analysis="0.300"/>
<oxide symbol="SiO2" formula="1.116100" analysis="53.500"/>
<oxide symbol="MgO" formula="0.917785" analysis="29.500"/>
<oxide symbol="Al2O3" formula="0.003688" analysis="0.300"/>
<oxide symbol="Fe2O3" formula="0.003918" analysis="0.500"/>
</chemistry>
</material>
<material name="Andafrac" weight="318.75" dfnumber="53" searchkey="" type="5" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.015957" analysis="0.400"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="32.000"/>
<oxide symbol="SiO2" formula="3.367824" analysis="63.500"/>
<oxide symbol="Fe2O3" formula="0.013945" analysis="0.700"/>
<oxide symbol="Na2O" formula="0.020565" analysis="0.400"/>
</chemistry>
</material>
<material name="Anhydrous Borax" weight="201.18818948735" dfnumber="58" searchkey="Calcined Borax, Dehydrated Borax, Pyrobor" type="15,17" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="30.820"/>
<oxide symbol="B2O3" formula="1.999830" analysis="69.190"/>
</chemistry>
</material>
<material name="APG Missouri Fireclay" weight="327.92316056542" dfnumber="1032" searchkey="AP Green, A.P., A. P., APG Fire, APGFC" type="9,14" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.082361" analysis="2.000"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="31.000"/>
<oxide symbol="CaO" formula="0.020528" analysis="0.350"/>
<oxide symbol="SiO2" formula="2.846868" analysis="52.000"/>
<oxide symbol="K2O" formula="0.017465" analysis="0.500"/>
<oxide symbol="Fe2O3" formula="0.041129" analysis="2.000"/>
<oxide symbol="MgO" formula="0.028576" analysis="0.350"/>
<oxide symbol="Na2O" formula="0.026535" analysis="0.500"/>
</chemistry>
</material>
<material name="Applewood Ash" weight="84.141416110555" dfnumber="65" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="0.028844" analysis="2.060"/>
<oxide symbol="CaO" formula="0.812126" analysis="54.140"/>
<oxide symbol="K2O" formula="0.080490" analysis="9.010"/>
<oxide symbol="MgO" formula="0.087703" analysis="4.200"/>
<oxide symbol="Na2O" formula="0.019681" analysis="1.450"/>
<oxide symbol="P2O5" formula="0.020341" analysis="3.430"/>
</chemistry>
</material>
<material name="Australian Spodumene" weight="385.23610346098" dfnumber="2275" searchkey="Ausi Spodumene, Ausi Spod" type="13" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.009381" analysis="0.150"/>
<oxide symbol="Al2O3" formula="1.007420" analysis="26.500"/>
<oxide symbol="P2O5" formula="0.004645" analysis="0.170"/>
<oxide symbol="MnO" formula="0.001094" analysis="0.020"/>
<oxide symbol="CaO" formula="0.003456" analysis="0.050"/>
<oxide symbol="Fe2O3" formula="0.001696" analysis="0.070"/>
<oxide symbol="SiO2" formula="4.161501" analysis="64.500"/>
<oxide symbol="Li2O" formula="0.988922" analysis="7.600"/>
<oxide symbol="K2O" formula="0.003293" analysis="0.080"/>
<oxide symbol="TiO2" formula="0.000485" analysis="0.010"/>
</chemistry>
</material>
<material name="Ball Clay" weight="407.53636363636" dfnumber="80" searchkey="" type="7,17" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.051064" analysis="1.000"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="25.000"/>
<oxide symbol="CaO" formula="0.021818" analysis="0.300"/>
<oxide symbol="SiO2" formula="4.005324" analysis="59.000"/>
<oxide symbol="K2O" formula="0.038981" analysis="0.900"/>
<oxide symbol="Fe2O3" formula="0.025500" analysis="1.000"/>
<oxide symbol="MgO" formula="0.030372" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.026323" analysis="0.400"/>
</chemistry>
</material>
<material name="Barium Carbonate" weight="197.39891836209" dfnumber="86" searchkey="Barium Carb, Witherite" type="15,17" property1="0">
<chemistry>
<oxide symbol="BaO" formula="1.000000" analysis="77.660"/>
</chemistry>
</material>
<material name="Barnard Slip" weight="1342.2516373823" dfnumber="90" searchkey="Blackbird Slip, Blackbird Clay, Barnard Clay" type="9" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="10.495665" analysis="47.000"/>
<oxide symbol="K2O" formula="0.156721" analysis="1.100"/>
<oxide symbol="Fe2O3" formula="2.843586" analysis="33.900"/>
<oxide symbol="MgO" formula="0.233120" analysis="0.700"/>
<oxide symbol="Na2O" formula="0.129881" analysis="0.600"/>
<oxide symbol="TiO2" formula="0.033595" analysis="0.200"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="7.600"/>
<oxide symbol="CaO" formula="0.143541" analysis="0.600"/>
</chemistry>
</material>
<material name="Bell Dark Ball Clay" weight="383.56711426147" dfnumber="95" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.012277" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.100032" analysis="2.100"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="26.800"/>
<oxide symbol="CaO" formula="0.013569" analysis="0.200"/>
<oxide symbol="SiO2" formula="3.729977" analysis="58.900"/>
<oxide symbol="K2O" formula="0.028282" analysis="0.700"/>
<oxide symbol="Fe2O3" formula="0.026166" analysis="1.100"/>
<oxide symbol="MgO" formula="0.037776" analysis="0.400"/>
</chemistry>
</material>
<material name="Bell Feldspar" weight="610.29946533922" dfnumber="96" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.652632" analysis="10.073"/>
<oxide symbol="Na2O" formula="0.304178" analysis="3.090"/>
<oxide symbol="Al2O3" formula="1.069383" analysis="17.872"/>
<oxide symbol="SiO2" formula="6.933422" analysis="68.275"/>
<oxide symbol="Fe2O3" formula="0.003013" analysis="0.079"/>
<oxide symbol="CaO" formula="0.043190" analysis="0.397"/>
</chemistry>
</material>
<material name="Bentolite L" weight="935.14297149844" dfnumber="104" searchkey="Bentolite" type="9" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.030166" analysis="0.200"/>
<oxide symbol="SiO2" formula="11.311962" analysis="72.700"/>
<oxide symbol="K2O" formula="0.009927" analysis="0.100"/>
<oxide symbol="MgO" formula="0.626523" analysis="2.700"/>
<oxide symbol="TiO2" formula="0.023408" analysis="0.200"/>
<oxide symbol="Al2O3" formula="1.256025" analysis="13.700"/>
<oxide symbol="Fe2O3" formula="0.040913" analysis="0.700"/>
<oxide symbol="CaO" formula="0.333384" analysis="2.000"/>
</chemistry>
</material>
<material name="Bentonite" weight="786.3961695332" dfnumber="106" searchkey="Montmorillonite, Bentonite USA" type="8,9,17,21" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.083948" analysis="1.000"/>
<oxide symbol="Al2O3" formula="1.550568" analysis="20.000"/>
<oxide symbol="SiO2" formula="7.763158" analysis="59.000"/>
<oxide symbol="CaO" formula="0.140961" analysis="1.000"/>
<oxide symbol="Fe2O3" formula="0.172985" analysis="3.500"/>
<oxide symbol="Na2O" formula="0.382640" analysis="3.000"/>
<oxide symbol="MgO" formula="0.392451" analysis="2.000"/>
</chemistry>
</material>
<material name="Blyth Frit 3104" weight="315.91870978573" dfnumber="2196" searchkey="F3104, Blyth F3104" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.658164" analysis="14.500"/>
<oxide symbol="K2O" formula="0.013415" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.310823" analysis="6.100"/>
<oxide symbol="Al2O3" formula="0.309724" analysis="10.000"/>
<oxide symbol="SiO2" formula="2.996234" analysis="57.000"/>
<oxide symbol="CaO" formula="0.675762" analysis="12.000"/>
</chemistry>
</material>
<material name="Bonding Clay" weight="346.55285918594" dfnumber="196" searchkey="" type="9" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="3.157662" analysis="54.700"/>
<oxide symbol="K2O" formula="0.062611" analysis="1.700"/>
<oxide symbol="Fe2O3" formula="0.036862" analysis="1.700"/>
<oxide symbol="MgO" formula="0.025827" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.011192" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.069475" analysis="1.600"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="29.400"/>
<oxide symbol="CaO" formula="0.012369" analysis="0.200"/>
</chemistry>
</material>
<material name="Bone Ash" weight="100.50161232533" dfnumber="123" searchkey="Calcium Phosphate" type="15,17,23" property1="0">
<chemistry>
<oxide symbol="P2O5" formula="0.300230" analysis="42.390"/>
<oxide symbol="CaO" formula="1.000000" analysis="55.820"/>
</chemistry>
</material>
<material name="Boraq" weight="106.39724181884" dfnumber="124" searchkey="Boraq 1" type="15" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.457996" analysis="30.000"/>
<oxide symbol="Al2O3" formula="0.029168" analysis="2.800"/>
<oxide symbol="CaO" formula="0.412898" analysis="21.800"/>
<oxide symbol="SiO2" formula="0.238676" analysis="13.500"/>
<oxide symbol="K2O" formula="0.006768" analysis="0.600"/>
<oxide symbol="Fe2O3" formula="0.001328" analysis="0.200"/>
<oxide symbol="MgO" formula="0.060642" analysis="2.300"/>
<oxide symbol="Na2O" formula="0.061696" analysis="3.600"/>
</chemistry>
</material>
<material name="Boraq 2" weight="102.06572521119" dfnumber="125" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.000638" analysis="0.100"/>
<oxide symbol="MgO" formula="0.091175" analysis="3.600"/>
<oxide symbol="Na2O" formula="0.052679" analysis="3.200"/>
<oxide symbol="B2O3" formula="0.388612" analysis="26.500"/>
<oxide symbol="Al2O3" formula="0.024015" analysis="2.400"/>
<oxide symbol="CaO" formula="0.462116" analysis="25.400"/>
<oxide symbol="SiO2" formula="0.202094" analysis="11.900"/>
<oxide symbol="K2O" formula="0.005418" analysis="0.500"/>
</chemistry>
</material>
<material name="Boraq 3" weight="102.6077090574" dfnumber="126" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.390940" analysis="26.500"/>
<oxide symbol="Al2O3" formula="0.024159" analysis="2.400"/>
<oxide symbol="CaO" formula="0.499659" analysis="27.300"/>
<oxide symbol="SiO2" formula="0.203304" analysis="11.900"/>
<oxide symbol="K2O" formula="0.005450" analysis="0.500"/>
<oxide symbol="Fe2O3" formula="0.000642" analysis="0.100"/>
<oxide symbol="MgO" formula="0.050956" analysis="2.000"/>
<oxide symbol="Na2O" formula="0.052995" analysis="3.200"/>
</chemistry>
</material>
<material name="Borax Decahydrate" weight="381.23158272689" dfnumber="2271" searchkey="Sodium TetraBorate Decahydrate, Borax 10-hydrate, 10 Mol Borax, Neobor" type="15,17" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="16.260"/>
<oxide symbol="B2O3" formula="2.000749" analysis="36.520"/>
</chemistry>
</material>
<material name="Borax Pentahydrate" weight="291.17438936769" dfnumber="128" searchkey="Borax 5 Mol, Sodium Tetraborate, Borax 5-hydrate" type="15,17" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="21.290"/>
<oxide symbol="B2O3" formula="2.000022" analysis="47.800"/>
</chemistry>
</material>
<material name="Boric Acid" weight="123.40425531915" dfnumber="129" searchkey="Boracic acid, Orthoboric Acid, Hydrous Boric Oxide" type="15,17" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.000000" analysis="56.310"/>
</chemistry>
</material>
<material name="Boric Oxide" weight="69.6" dfnumber="2273" searchkey="Anhydrous Boric Acid, B2O3" type="15,17" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="C &amp; C Ball Clay" weight="387.9802206162" dfnumber="152" searchkey="C&amp;C Ball Clay, C and C Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.079635" analysis="1.640"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="26.290"/>
<oxide symbol="CaO" formula="0.006916" analysis="0.100"/>
<oxide symbol="SiO2" formula="3.863018" analysis="59.840"/>
<oxide symbol="K2O" formula="0.016887" analysis="0.410"/>
<oxide symbol="Fe2O3" formula="0.022309" analysis="0.920"/>
<oxide symbol="MgO" formula="0.019255" analysis="0.200"/>
<oxide symbol="Na2O" formula="0.012515" analysis="0.200"/>
</chemistry>
</material>
<material name="Cadycal" weight="219.00150850103" dfnumber="165" searchkey="Cadycal Jan/00" type="15" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.000674" analysis="0.050"/>
<oxide symbol="Al2O3" formula="0.002115" analysis="0.100"/>
<oxide symbol="B2O3" formula="1.472563" analysis="47.500"/>
<oxide symbol="SiO2" formula="0.017951" analysis="0.500"/>
<oxide symbol="CaO" formula="1.000000" analysis="26.000"/>
<oxide symbol="MgO" formula="0.012850" analysis="0.240"/>
<oxide symbol="K2O" formula="0.000229" analysis="0.010"/>
<oxide symbol="Na2O" formula="0.003480" analysis="0.100"/>
<oxide symbol="SrO" formula="0.000625" analysis="0.030"/>
</chemistry>
</material>
<material name="Calcined Alumina" weight="102" dfnumber="41" searchkey="Alumina Calcined, Calcnd Alum, Ground Alumina, Corundum" type="4,17,20" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Calcined Kaolin" weight="222.22222222222" dfnumber="167" searchkey="Cal Kaolin, Meta Kaolin" type="17,18,20,24" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="45.900"/>
<oxide symbol="SiO2" formula="2.000370" analysis="54.100"/>
</chemistry>
</material>
<material name="Calcium Borate" weight="125.70020165808" dfnumber="171" searchkey="Anhydrous Borocalcite" type="15,17" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.000003" analysis="55.370"/>
<oxide symbol="CaO" formula="1.000000" analysis="44.630"/>
</chemistry>
</material>
<material name="Calcium Carbonate" weight="100" dfnumber="173" searchkey="Carbonate of Lime, Whiting, Aragonite, Calcite, CaCO3" type="15,17" property1="0">
<chemistry>
<oxide symbol="CaO" formula="1.000000" analysis="56.100"/>
</chemistry>
</material>
<material name="Calcium Feldspar" weight="518.4842883549" dfnumber="175" searchkey="Lime Spar, Lime Feldspar, Ca-Feldspar" type="13,17" property1="0">
<chemistry>
<oxide symbol="CaO" formula="1.000000" analysis="10.820"/>
<oxide symbol="Al2O3" formula="0.999353" analysis="19.660"/>
<oxide symbol="SiO2" formula="5.997509" analysis="69.520"/>
</chemistry>
</material>
<material name="Calvert Clay" weight="428.57142857143" dfnumber="184" searchkey="" type="9" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.022918" analysis="0.300"/>
<oxide symbol="SiO2" formula="4.120989" analysis="57.790"/>
<oxide symbol="K2O" formula="0.090992" analysis="2.000"/>
<oxide symbol="Fe2O3" formula="0.152946" analysis="5.710"/>
<oxide symbol="MgO" formula="0.085076" analysis="0.800"/>
<oxide symbol="Na2O" formula="0.028341" analysis="0.410"/>
<oxide symbol="TiO2" formula="0.064903" analysis="1.210"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="23.800"/>
</chemistry>
</material>
<material name="Camadil 95 Dolomite" weight="92.250335558673" dfnumber="2159" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.000918" analysis="0.100"/>
<oxide symbol="CaO" formula="0.500590" analysis="30.000"/>
<oxide symbol="MgO" formula="0.499410" analysis="21.500"/>
<oxide symbol="SiO2" formula="0.005919" analysis="0.380"/>
<oxide symbol="Fe2O3" formula="0.001463" analysis="0.250"/>
</chemistry>
</material>
<material name="Carbondale Clay" weight="531.36412711178" dfnumber="186" searchkey="Carbondale Red Clay" type="9" property1="0">
<chemistry>
<oxide symbol="P2O5" formula="0.003376" analysis="0.090"/>
<oxide symbol="MgO" formula="0.084543" analysis="0.640"/>
<oxide symbol="SiO2" formula="4.958646" analysis="55.980"/>
<oxide symbol="Na2O" formula="0.050660" analysis="0.590"/>
<oxide symbol="Cr2O3" formula="0.001051" analysis="0.030"/>
<oxide symbol="SrO" formula="0.000514" analysis="0.010"/>
<oxide symbol="BaO" formula="0.004862" analysis="0.140"/>
<oxide symbol="Fe2O3" formula="0.399935" analysis="12.020"/>
<oxide symbol="TiO2" formula="0.068627" analysis="1.030"/>
<oxide symbol="CaO" formula="0.053141" analysis="0.560"/>
<oxide symbol="MnO" formula="0.002253" analysis="0.030"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="19.160"/>
<oxide symbol="K2O" formula="0.028822" analysis="0.510"/>
</chemistry>
</material>
<material name="Cedar Heights Fireclay" weight="462.37533998187" dfnumber="197" searchkey="" type="14" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.017939" analysis="0.310"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="22.060"/>
<oxide symbol="SiO2" formula="5.125365" analysis="66.620"/>
<oxide symbol="CaO" formula="0.046979" analysis="0.570"/>
<oxide symbol="Fe2O3" formula="0.049127" analysis="1.700"/>
<oxide symbol="MgO" formula="0.012621" analysis="0.110"/>
<oxide symbol="Na2O" formula="0.037288" analysis="0.500"/>
</chemistry>
</material>
<material name="Ceramic Rutile" weight="20397.96" dfnumber="968" searchkey="Calcined Rutile, Light Rutile, Rutile Ceramic" type="10,17,23" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="0.500"/>
<oxide symbol="SiO2" formula="2.715474" analysis="0.800"/>
<oxide symbol="Cr2O3" formula="0.268421" analysis="0.200"/>
<oxide symbol="Fe2O3" formula="0.637500" analysis="0.500"/>
<oxide symbol="TiO2" formula="245.336170" analysis="96.090"/>
<oxide symbol="V2O5" formula="0.785047" analysis="0.700"/>
<oxide symbol="ZrO" formula="2.283582" analysis="1.200"/>
</chemistry>
</material>
<material name="Ceramitalc" weight="118.16080204449" dfnumber="204" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.116847" analysis="56.800"/>
<oxide symbol="Fe2O3" formula="0.001477" analysis="0.200"/>
<oxide symbol="CaO" formula="0.146190" analysis="6.940"/>
<oxide symbol="MnO" formula="0.002167" analysis="0.130"/>
<oxide symbol="MgO" formula="0.850380" analysis="29.000"/>
<oxide symbol="Na2O" formula="0.003431" analysis="0.180"/>
<oxide symbol="Al2O3" formula="0.003244" analysis="0.280"/>
</chemistry>
</material>
<material name="Champion-Challenger" weight="360.59690493203" dfnumber="211" searchkey="Champion Challenger Ball Clay, Chalenger" type="7" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.022014" analysis="0.980"/>
<oxide symbol="Na2O" formula="0.006956" analysis="0.120"/>
<oxide symbol="MnO" formula="0.001014" analysis="0.020"/>
<oxide symbol="TiO2" formula="0.073771" analysis="1.640"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="28.380"/>
<oxide symbol="CaO" formula="0.023704" analysis="0.370"/>
<oxide symbol="P2O5" formula="0.003799" analysis="0.150"/>
<oxide symbol="K2O" formula="0.015261" analysis="0.400"/>
<oxide symbol="SiO2" formula="3.324973" analysis="55.600"/>
<oxide symbol="MgO" formula="0.026755" analysis="0.300"/>
</chemistry>
</material>
<material name="Cherry Ash" weight="97.219092668243" dfnumber="2348" searchkey="Cherry Wood Ash, Cherry Ash Washed" type="15,17" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.289486" analysis="12.000"/>
<oxide symbol="CaO" formula="0.710514" analysis="41.000"/>
<oxide symbol="Fe2O3" formula="0.021267" analysis="3.500"/>
<oxide symbol="SiO2" formula="0.541903" analysis="33.500"/>
<oxide symbol="P2O5" formula="0.068512" analysis="10.000"/>
</chemistry>
</material>
<material name="Chesterfield Feldspar" weight="640.7586163805" dfnumber="212" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.026470" analysis="16.340"/>
<oxide symbol="SiO2" formula="7.543040" analysis="70.750"/>
<oxide symbol="Fe2O3" formula="0.002803" analysis="0.070"/>
<oxide symbol="CaO" formula="0.034265" analysis="0.300"/>
<oxide symbol="K2O" formula="0.578179" analysis="8.500"/>
<oxide symbol="Na2O" formula="0.387556" analysis="3.750"/>
</chemistry>
</material>
<material name="Chrome Oxide" weight="152" dfnumber="218" searchkey="Chromium (III) Oxide, Cr2O3, Chromium Oxide" type="10,17" property1="0">
<chemistry>
<oxide symbol="Cr2O3" formula="1.000000" analysis="131.580"/>
</chemistry>
</material>
<material name="CMC Gum" weight="0" dfnumber="228" searchkey="C.M.C." type="2" property1="0"/>
<material name="Cobalt Carbonate" weight="118.92063492063" dfnumber="229" searchkey="Spherocobaltite, CoCO3, Cobalt(II) carbonate" type="10,17" property1="0">
<chemistry>
<oxide symbol="CoO" formula="1.000000" analysis="63.000"/>
</chemistry>
</material>
<material name="Cobalt Oxide" weight="80.257096946974" dfnumber="230" searchkey="Cobalt(II) oxide, Cobaltosic Oxide, CoO, cobaltous oxide" type="10,17" property1="0">
<chemistry>
<oxide symbol="CoO" formula="1.000000" analysis="93.350"/>
</chemistry>
</material>
<material name="Colemanite" weight="205.49450549451" dfnumber="231" searchkey="" type="15,17" property1="0">
<chemistry>
<oxide symbol="CaO" formula="1.000000" analysis="27.300"/>
<oxide symbol="B2O3" formula="1.499874" analysis="50.800"/>
</chemistry>
</material>
<material name="Copper Carbonate" weight="123.54768561665" dfnumber="235" searchkey="Synthetic Malachite, CuCO3" type="10,17" property1="0">
<chemistry>
<oxide symbol="CuO" formula="1.000000" analysis="64.400"/>
</chemistry>
</material>
<material name="Copper Oxide Black" weight="79.54" dfnumber="237" searchkey="Copper (II) Oxide, Black Copper, BCO, Cupric Oxide" type="10,17" property1="0">
<chemistry>
<oxide symbol="CuO" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Copper Oxide Red" weight="143" dfnumber="238" searchkey="Cu2O, Red Copper, RCO, Copper (I) Oxide, Cuprous Oxide" type="10,17" property1="0">
<chemistry>
<oxide symbol="Cu2O" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Cornwall Stone" weight="742.80636240776" dfnumber="240" searchkey="Cornish Stone, China Stone, Corn Stn, China-stone" type="13,17" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="9.117284" analysis="73.760"/>
<oxide symbol="CaO" formula="0.239682" analysis="1.810"/>
<oxide symbol="Fe2O3" formula="0.009286" analysis="0.200"/>
<oxide symbol="K2O" formula="0.339107" analysis="4.300"/>
<oxide symbol="MgO" formula="0.025807" analysis="0.140"/>
<oxide symbol="Na2O" formula="0.395404" analysis="3.300"/>
<oxide symbol="TiO2" formula="0.013946" analysis="0.150"/>
<oxide symbol="Al2O3" formula="1.189337" analysis="16.330"/>
</chemistry>
</material>
<material name="Cryolite" weight="171.92371925073" dfnumber="250" searchkey="Cryloite, Sodium Fluoaluminate, Kryolith" type="15,17" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="44.310"/>
<oxide symbol="Al2O3" formula="0.332661" analysis="24.250"/>
<oxide symbol="F" formula="3.999596" analysis="54.310"/>
</chemistry>
</material>
<material name="Custer Feldspar" weight="623.85466887151" dfnumber="253" searchkey="Custer Spar" type="13" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.005863" analysis="0.150"/>
<oxide symbol="CaO" formula="0.033445" analysis="0.300"/>
<oxide symbol="K2O" formula="0.663931" analysis="10.000"/>
<oxide symbol="Na2O" formula="0.302624" analysis="3.000"/>
<oxide symbol="Al2O3" formula="1.042372" analysis="17.000"/>
<oxide symbol="SiO2" formula="7.180396" analysis="69.000"/>
</chemistry>
</material>
<material name="DF Cornwall Stone" weight="936.16548633137" dfnumber="265" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="12.395702" analysis="79.570"/>
<oxide symbol="Fe2O3" formula="0.003511" analysis="0.060"/>
<oxide symbol="CaO" formula="0.033378" analysis="0.200"/>
<oxide symbol="K2O" formula="0.377684" analysis="3.800"/>
<oxide symbol="Na2O" formula="0.588937" analysis="3.900"/>
<oxide symbol="Al2O3" formula="1.102400" analysis="12.010"/>
</chemistry>
</material>
<material name="Diamond Kaolin" weight="267.91587231382" dfnumber="266" searchkey="" type="18" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.047157" analysis="1.400"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.900"/>
<oxide symbol="CaO" formula="0.007196" analysis="0.150"/>
<oxide symbol="SiO2" formula="2.041979" analysis="45.600"/>
<oxide symbol="K2O" formula="0.005143" analysis="0.180"/>
<oxide symbol="Fe2O3" formula="0.011774" analysis="0.700"/>
<oxide symbol="MgO" formula="0.006678" analysis="0.100"/>
<oxide symbol="Na2O" formula="0.003473" analysis="0.080"/>
</chemistry>
</material>
<material name="Dolomite" weight="183.99475237783" dfnumber="273" searchkey="Calcium Magnesium Carbonate, Raw Limestone" type="15,17" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.999872" analysis="21.900"/>
<oxide symbol="Al2O3" formula="0.000000" analysis="0.000"/>
<oxide symbol="CaO" formula="1.000000" analysis="30.490"/>
</chemistry>
</material>
<material name="English Kaolin" weight="272.87319422151" dfnumber="289" searchkey="" type="17,18" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.002201" analysis="0.050"/>
<oxide symbol="TiO2" formula="0.002049" analysis="0.060"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.380"/>
<oxide symbol="CaO" formula="0.000973" analysis="0.020"/>
<oxide symbol="SiO2" formula="2.153928" analysis="47.440"/>
<oxide symbol="K2O" formula="0.051852" analysis="1.790"/>
<oxide symbol="Fe2O3" formula="0.013985" analysis="0.820"/>
<oxide symbol="MgO" formula="0.018959" analysis="0.280"/>
</chemistry>
</material>
<material name="EP Kaolin" weight="272.92312711754" dfnumber="291" searchkey="EPK, Edgar Plastic Kaolin, EPK Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="P2O5" formula="0.004618" analysis="0.240"/>
<oxide symbol="K2O" formula="0.009564" analysis="0.330"/>
<oxide symbol="SiO2" formula="2.077400" analysis="45.730"/>
<oxide symbol="MgO" formula="0.006775" analysis="0.100"/>
<oxide symbol="Fe2O3" formula="0.013480" analysis="0.790"/>
<oxide symbol="Na2O" formula="0.002642" analysis="0.060"/>
<oxide symbol="TiO2" formula="0.012643" analysis="0.370"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.360"/>
<oxide symbol="CaO" formula="0.008760" analysis="0.180"/>
</chemistry>
</material>
<material name="Eureka Feldspar" weight="640.83157540813" dfnumber="296" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.360979" analysis="3.490"/>
<oxide symbol="Al2O3" formula="1.071946" analysis="17.050"/>
<oxide symbol="SiO2" formula="7.437157" analysis="69.700"/>
<oxide symbol="Fe2O3" formula="0.004409" analysis="0.110"/>
<oxide symbol="CaO" formula="0.001143" analysis="0.010"/>
<oxide symbol="K2O" formula="0.637878" analysis="9.370"/>
</chemistry>
</material>
<material name="F-2 Ball Clay" weight="453.53490440196" dfnumber="302" searchkey="Hick F-2, F2 Ball Clay, Old Hickory F-2 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.123588" analysis="4.360"/>
<oxide symbol="MgO" formula="0.132797" analysis="1.180"/>
<oxide symbol="Na2O" formula="0.013167" analysis="0.180"/>
<oxide symbol="TiO2" formula="0.070954" analysis="1.250"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="22.490"/>
<oxide symbol="CaO" formula="0.031529" analysis="0.390"/>
<oxide symbol="SiO2" formula="4.551951" analysis="60.320"/>
<oxide symbol="K2O" formula="0.081848" analysis="1.700"/>
</chemistry>
</material>
<material name="F-20 Feldspar" weight="557.31542842972" dfnumber="307" searchkey="F20 Feldspar" type="13" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.035433" analysis="18.850"/>
<oxide symbol="SiO2" formula="6.353341" analysis="68.150"/>
<oxide symbol="Fe2O3" formula="0.002451" analysis="0.070"/>
<oxide symbol="CaO" formula="0.139822" analysis="1.400"/>
<oxide symbol="K2O" formula="0.243862" analysis="4.100"/>
<oxide symbol="Na2O" formula="0.616316" analysis="6.820"/>
</chemistry>
</material>
<material name="F-4 Feldspar" weight="516.48928424787" dfnumber="303" searchkey="F4 Feldspar, Kona Feldspar, Kona F4, F4 Spar, F 4 Feldspar" type="13" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.991575" analysis="19.600"/>
<oxide symbol="SiO2" formula="5.735507" analysis="66.800"/>
<oxide symbol="CaO" formula="0.156371" analysis="1.700"/>
<oxide symbol="Fe2O3" formula="0.001290" analysis="0.040"/>
<oxide symbol="K2O" formula="0.262942" analysis="4.800"/>
<oxide symbol="MgO" formula="0.006402" analysis="0.050"/>
<oxide symbol="Na2O" formula="0.574285" analysis="6.900"/>
</chemistry>
</material>
<material name="Ferro Frit 3110" weight="260.76313213502" dfnumber="349" searchkey="F3110, Frit KFG 4110, Ferro Crystal Frit" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.097412" analysis="2.600"/>
<oxide symbol="Al2O3" formula="0.094591" analysis="3.700"/>
<oxide symbol="SiO2" formula="3.028497" analysis="69.800"/>
<oxide symbol="CaO" formula="0.292836" analysis="6.300"/>
<oxide symbol="K2O" formula="0.063668" analysis="2.300"/>
<oxide symbol="Na2O" formula="0.643496" analysis="15.300"/>
</chemistry>
</material>
<material name="Ferro Frit 3124" weight="282.18459593299" dfnumber="350" searchkey="F3124" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.273611" analysis="9.900"/>
<oxide symbol="K2O" formula="0.020948" analysis="0.700"/>
<oxide symbol="SiO2" formula="2.589189" analysis="55.200"/>
<oxide symbol="B2O3" formula="0.558945" analysis="13.800"/>
<oxide symbol="CaO" formula="0.713550" analysis="14.200"/>
<oxide symbol="Na2O" formula="0.286450" analysis="6.300"/>
</chemistry>
</material>
<material name="Ferro Frit 3134" weight="190.6876531636" dfnumber="351" searchkey="F3134" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.683212" analysis="20.100"/>
<oxide symbol="B2O3" formula="0.632886" analysis="23.100"/>
<oxide symbol="SiO2" formula="1.475370" analysis="46.500"/>
<oxide symbol="Na2O" formula="0.316788" analysis="10.300"/>
</chemistry>
</material>
<material name="Ferro Frit 3185" weight="805.19480519481" dfnumber="353" searchkey="F3185" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="7.700"/>
<oxide symbol="B2O3" formula="4.419316" analysis="38.200"/>
<oxide symbol="SiO2" formula="7.248093" analysis="54.100"/>
</chemistry>
</material>
<material name="Ferro Frit 3191" weight="248.84349517008" dfnumber="354" searchkey="F3191" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.000022" analysis="27.970"/>
<oxide symbol="SiO2" formula="1.999857" analysis="48.300"/>
<oxide symbol="CaO" formula="0.499905" analysis="11.270"/>
<oxide symbol="Na2O" formula="0.500095" analysis="12.460"/>
</chemistry>
</material>
<material name="Ferro Frit 3195" weight="337.57920847328" dfnumber="356" searchkey="F3195" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.410018" analysis="12.390"/>
<oxide symbol="SiO2" formula="2.664419" analysis="47.440"/>
<oxide symbol="CaO" formula="0.673888" analysis="11.200"/>
<oxide symbol="Na2O" formula="0.326112" analysis="5.990"/>
<oxide symbol="B2O3" formula="1.114967" analysis="22.990"/>
</chemistry>
</material>
<material name="Ferro Frit 3211" weight="133.57142857143" dfnumber="357" searchkey="F3211" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="1.000000" analysis="42.000"/>
<oxide symbol="B2O3" formula="1.113095" analysis="58.000"/>
</chemistry>
</material>
<material name="Ferro Frit 3227" weight="373.52741784878" dfnumber="363" searchkey="F3227 Frit, F3227" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.529530" analysis="28.500"/>
<oxide symbol="Al2O3" formula="0.571277" analysis="15.600"/>
<oxide symbol="SiO2" formula="2.355522" analysis="37.900"/>
<oxide symbol="K2O" formula="0.162576" analysis="4.100"/>
<oxide symbol="Na2O" formula="0.837424" analysis="13.900"/>
</chemistry>
</material>
<material name="Ferro Frit 3249" weight="273.88396913274" dfnumber="369" searchkey="F3249 Frit, F3249 (Ferro)" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.137248" analysis="28.900"/>
<oxide symbol="Al2O3" formula="0.357123" analysis="13.300"/>
<oxide symbol="SiO2" formula="1.918555" analysis="42.100"/>
<oxide symbol="CaO" formula="0.170872" analysis="3.500"/>
<oxide symbol="MgO" formula="0.829128" analysis="12.200"/>
</chemistry>
</material>
<material name="Ferro Frit 3269" weight="358.31112713011" dfnumber="371" searchkey="F3269" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.641493" analysis="11.100"/>
<oxide symbol="ZnO" formula="0.044019" analysis="1.000"/>
<oxide symbol="B2O3" formula="0.782519" analysis="15.200"/>
<oxide symbol="Al2O3" formula="0.463697" analysis="13.200"/>
<oxide symbol="CaO" formula="0.006387" analysis="0.100"/>
<oxide symbol="SiO2" formula="2.963072" analysis="49.700"/>
<oxide symbol="K2O" formula="0.308102" analysis="8.100"/>
<oxide symbol="F" formula="0.301736" analysis="1.600"/>
</chemistry>
</material>
<material name="Ferro Frit 3278" weight="270.4392246507" dfnumber="376" searchkey="F3278" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.332626" analysis="6.900"/>
<oxide symbol="Na2O" formula="0.667374" analysis="15.300"/>
<oxide symbol="B2O3" formula="0.839294" analysis="21.600"/>
<oxide symbol="SiO2" formula="2.528899" analysis="56.200"/>
</chemistry>
</material>
<material name="Ferro Frit 3289" weight="373.90979366235" dfnumber="382" searchkey="F3289" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.331694" analysis="5.500"/>
<oxide symbol="B2O3" formula="0.666161" analysis="12.400"/>
<oxide symbol="Al2O3" formula="0.197952" analysis="5.400"/>
<oxide symbol="SiO2" formula="3.067180" analysis="49.300"/>
<oxide symbol="BaO" formula="0.668306" analysis="27.400"/>
</chemistry>
</material>
<material name="Ferro Frit 3292" weight="292.75959159865" dfnumber="384" searchkey="F3292" type="16" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.096343" analysis="3.100"/>
<oxide symbol="Al2O3" formula="0.309981" analysis="10.800"/>
<oxide symbol="Li2O" formula="0.039297" analysis="0.400"/>
<oxide symbol="SiO2" formula="2.995793" analysis="61.500"/>
<oxide symbol="MgO" formula="0.050852" analysis="0.700"/>
<oxide symbol="Na2O" formula="0.141658" analysis="3.000"/>
<oxide symbol="SrO" formula="0.118686" analysis="4.200"/>
<oxide symbol="CaO" formula="0.553164" analysis="10.600"/>
<oxide symbol="B2O3" formula="0.239760" analysis="5.700"/>
</chemistry>
</material>
<material name="Ferro Frit 3300" weight="207.92291460667" dfnumber="387" searchkey="F3300" type="16,19" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.342331" analysis="38.800"/>
<oxide symbol="MgO" formula="0.020638" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.023475" analysis="0.700"/>
<oxide symbol="PbO" formula="0.206805" analysis="22.200"/>
<oxide symbol="BaO" formula="0.084091" analysis="6.200"/>
<oxide symbol="ZnO" formula="0.268205" analysis="10.500"/>
<oxide symbol="CaO" formula="0.326154" analysis="8.800"/>
<oxide symbol="Al2O3" formula="0.187538" analysis="9.200"/>
<oxide symbol="K2O" formula="0.070632" analysis="3.200"/>
</chemistry>
</material>
<material name="Ferro Frit 3304" weight="382.45373543523" dfnumber="389" searchkey="F3304" type="16,19" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.067855" analysis="1.100"/>
<oxide symbol="PbO" formula="0.932145" analysis="54.400"/>
<oxide symbol="Al2O3" formula="0.149982" analysis="4.000"/>
<oxide symbol="SiO2" formula="2.577267" analysis="40.500"/>
</chemistry>
</material>
<material name="Ferro Frit 3327" weight="262.58823529412" dfnumber="390" searchkey="F3327" type="16,19" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="0.655378" analysis="15.000"/>
<oxide symbol="PbO" formula="1.000000" analysis="85.000"/>
</chemistry>
</material>
<material name="Ferro Frit 3419" weight="271.40077821012" dfnumber="398" searchkey="F3419" type="16,19" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.280156" analysis="6.400"/>
<oxide symbol="PbO" formula="0.719844" analysis="59.200"/>
<oxide symbol="B2O3" formula="0.565418" analysis="14.500"/>
<oxide symbol="SiO2" formula="0.898648" analysis="19.900"/>
</chemistry>
</material>
<material name="Ferro Frit 3467" weight="343.29495724698" dfnumber="409" searchkey="F3467" type="16,19" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.221914" analysis="4.500"/>
<oxide symbol="CaO" formula="0.489449" analysis="8.000"/>
<oxide symbol="Al2O3" formula="0.305539" analysis="9.080"/>
<oxide symbol="K2O" formula="0.061941" analysis="1.700"/>
<oxide symbol="SiO2" formula="3.228383" analysis="56.530"/>
<oxide symbol="MgO" formula="0.051101" analysis="0.600"/>
<oxide symbol="Na2O" formula="0.132862" analysis="2.400"/>
<oxide symbol="PbO" formula="0.264647" analysis="17.210"/>
</chemistry>
</material>
<material name="Ferro Frit 3481" weight="293.3204788365" dfnumber="413" searchkey="F3481" type="16,19" property1="0">
<chemistry>
<oxide symbol="PbO" formula="0.299204" analysis="22.770"/>
<oxide symbol="B2O3" formula="0.261265" analysis="6.200"/>
<oxide symbol="Al2O3" formula="0.201278" analysis="7.000"/>
<oxide symbol="CaO" formula="0.517573" analysis="9.900"/>
<oxide symbol="SiO2" formula="2.433194" analysis="49.860"/>
<oxide symbol="K2O" formula="0.037051" analysis="1.190"/>
<oxide symbol="Na2O" formula="0.146173" analysis="3.090"/>
</chemistry>
</material>
<material name="Ferro Frit 349" weight="312.87459354123" dfnumber="418" searchkey="" type="16,19" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="2.799941" analysis="53.784"/>
<oxide symbol="K2O" formula="0.090010" analysis="2.710"/>
<oxide symbol="Na2O" formula="0.089977" analysis="1.783"/>
<oxide symbol="PbO" formula="0.239997" analysis="17.121"/>
<oxide symbol="B2O3" formula="0.359986" analysis="8.008"/>
<oxide symbol="Al2O3" formula="0.189995" analysis="6.194"/>
<oxide symbol="CaO" formula="0.580017" analysis="10.400"/>
</chemistry>
</material>
<material name="Ferro Frit 3498" weight="341.80704441041" dfnumber="423" searchkey="F3498" type="16,19" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="65.300"/>
<oxide symbol="Al2O3" formula="0.083776" analysis="2.500"/>
<oxide symbol="SiO2" formula="1.831312" analysis="32.200"/>
</chemistry>
</material>
<material name="Ferro Frit 3602" weight="341.96414891987" dfnumber="434" searchkey="F3602" type="16,19" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.833861" analysis="32.230"/>
<oxide symbol="PbO" formula="1.000000" analysis="65.270"/>
<oxide symbol="Al2O3" formula="0.083815" analysis="2.500"/>
</chemistry>
</material>
<material name="Ferro Frit 5301" weight="305.83507744764" dfnumber="468" searchkey="F5301, Frit 501E34" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.362804" analysis="12.100"/>
<oxide symbol="SiO2" formula="2.264503" analysis="44.500"/>
<oxide symbol="CaO" formula="0.130839" analysis="2.400"/>
<oxide symbol="F" formula="1.448692" analysis="9.000"/>
<oxide symbol="K2O" formula="0.178566" analysis="5.500"/>
<oxide symbol="Na2O" formula="0.690595" analysis="14.000"/>
<oxide symbol="B2O3" formula="0.549273" analysis="12.500"/>
</chemistry>
</material>
<material name="Ferro Frit CC-257" weight="280.6881723203" dfnumber="491" searchkey="Frit CC257" type="6,16" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.077294" analysis="2.200"/>
<oxide symbol="CaO" formula="0.275212" analysis="5.500"/>
<oxide symbol="Al2O3" formula="0.254846" analysis="9.260"/>
<oxide symbol="K2O" formula="0.023542" analysis="0.790"/>
<oxide symbol="SiO2" formula="2.172865" analysis="46.520"/>
<oxide symbol="MgO" formula="0.021594" analysis="0.310"/>
<oxide symbol="Fe2O3" formula="0.000702" analysis="0.040"/>
<oxide symbol="Na2O" formula="0.045277" analysis="1.000"/>
<oxide symbol="SrO" formula="0.015445" analysis="0.570"/>
<oxide symbol="BaO" formula="0.618931" analysis="33.800"/>
</chemistry>
</material>
<material name="Fluorspar" weight="94.11204735376" dfnumber="317" searchkey="Fluorite, Calcium Fluoride, Blue John" type="15,17,23" property1="0">
<chemistry>
<oxide symbol="CaO" formula="1.000000" analysis="71.800"/>
<oxide symbol="F" formula="2.000634" analysis="48.650"/>
</chemistry>
</material>
<material name="Frit B300" weight="343.38461538462" dfnumber="484" searchkey="B-300" type="16,19" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="65.000"/>
<oxide symbol="Al2O3" formula="0.100995" analysis="3.000"/>
<oxide symbol="SiO2" formula="1.828337" analysis="32.000"/>
</chemistry>
</material>
<material name="Frit P2954" weight="211.69811320755" dfnumber="709" searchkey="PotteryCrafts Frit 2954" type="16" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.005253" analysis="0.100"/>
<oxide symbol="Na2O" formula="0.010243" analysis="0.300"/>
<oxide symbol="CaO" formula="1.000000" analysis="26.500"/>
<oxide symbol="B2O3" formula="1.529945" analysis="50.300"/>
<oxide symbol="Al2O3" formula="0.101698" analysis="4.900"/>
<oxide symbol="SiO2" formula="0.630515" analysis="17.900"/>
</chemistry>
</material>
<material name="Frit RCG 2430" weight="279.82432802487" dfnumber="2301" searchkey="F RCG 2430, RCG2430, RCG-2430" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.530701" analysis="13.200"/>
<oxide symbol="SiO2" formula="2.616660" analysis="56.200"/>
<oxide symbol="CaO" formula="0.693326" analysis="13.900"/>
<oxide symbol="K2O" formula="0.017823" analysis="0.600"/>
<oxide symbol="Na2O" formula="0.288851" analysis="6.400"/>
<oxide symbol="Al2O3" formula="0.266107" analysis="9.700"/>
</chemistry>
</material>
<material name="Fusion Frit F-12" weight="190.7493528715" dfnumber="511" searchkey="F12 Fusion,Frit F12" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.319967" analysis="10.400"/>
<oxide symbol="B2O3" formula="0.652275" analysis="23.800"/>
<oxide symbol="Al2O3" formula="0.014961" analysis="0.800"/>
<oxide symbol="SiO2" formula="1.428240" analysis="45.000"/>
<oxide symbol="CaO" formula="0.680033" analysis="20.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-13" weight="217.60666594938" dfnumber="513" searchkey="Frit F13" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.298332" analysis="8.500"/>
<oxide symbol="B2O3" formula="0.578409" analysis="18.500"/>
<oxide symbol="Al2O3" formula="0.096003" analysis="4.500"/>
<oxide symbol="SiO2" formula="1.823044" analysis="50.350"/>
<oxide symbol="CaO" formula="0.698203" analysis="18.000"/>
<oxide symbol="K2O" formula="0.003465" analysis="0.150"/>
</chemistry>
</material>
<material name="Fusion Frit F-134" weight="290.10005551245" dfnumber="514" searchkey="F134 Fusion" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.327074" analysis="11.500"/>
<oxide symbol="K2O" formula="0.036955" analysis="1.200"/>
<oxide symbol="SiO2" formula="2.920308" analysis="60.500"/>
<oxide symbol="Li2O" formula="0.038940" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.229273" analysis="4.900"/>
<oxide symbol="SrO" formula="0.126009" analysis="4.500"/>
<oxide symbol="B2O3" formula="0.250086" analysis="6.000"/>
<oxide symbol="CaO" formula="0.568824" analysis="11.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-18" weight="281.71240086677" dfnumber="517" searchkey="F18 Fusion, Frit F18, Frit F 18" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.360236" analysis="8.900"/>
<oxide symbol="Al2O3" formula="0.187808" analysis="6.800"/>
<oxide symbol="CaO" formula="0.592550" analysis="11.800"/>
<oxide symbol="SiO2" formula="2.789000" analysis="59.500"/>
<oxide symbol="K2O" formula="0.071774" analysis="2.400"/>
<oxide symbol="Na2O" formula="0.118137" analysis="2.600"/>
<oxide symbol="SrO" formula="0.217539" analysis="8.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-19" weight="273.207132197" dfnumber="518" searchkey="Frit F19, F19 Fusion" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.573107" analysis="14.600"/>
<oxide symbol="Al2O3" formula="0.259815" analysis="9.700"/>
<oxide symbol="SiO2" formula="2.477502" analysis="54.500"/>
<oxide symbol="CaO" formula="0.691540" analysis="14.200"/>
<oxide symbol="Na2O" formula="0.308460" analysis="7.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-2" weight="424.53313804467" dfnumber="519" searchkey="F2 Fusion" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.238222" analysis="20.300"/>
<oxide symbol="Al2O3" formula="0.561882" analysis="13.500"/>
<oxide symbol="SiO2" formula="3.461252" analysis="49.000"/>
<oxide symbol="K2O" formula="0.166749" analysis="3.700"/>
<oxide symbol="CaO" formula="0.794581" analysis="10.500"/>
<oxide symbol="Na2O" formula="0.205419" analysis="3.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-280" weight="268.8061217048" dfnumber="523" searchkey="F280 Fusion, Frit F280" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.303027" analysis="6.990"/>
<oxide symbol="Al2O3" formula="0.223719" analysis="8.490"/>
<oxide symbol="B2O3" formula="0.578879" analysis="14.990"/>
<oxide symbol="SiO2" formula="2.448530" analysis="54.750"/>
<oxide symbol="CaO" formula="0.679853" analysis="14.190"/>
<oxide symbol="K2O" formula="0.017120" analysis="0.600"/>
</chemistry>
</material>
<material name="Fusion Frit F-309" weight="189.5535640175" dfnumber="526" searchkey="Frit F309, F 309" type="16" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.202253" analysis="4.300"/>
<oxide symbol="Na2O" formula="0.189554" analysis="6.200"/>
<oxide symbol="B2O3" formula="1.225562" analysis="45.000"/>
<oxide symbol="Al2O3" formula="0.046459" analysis="2.500"/>
<oxide symbol="SiO2" formula="0.756953" analysis="24.000"/>
<oxide symbol="CaO" formula="0.608193" analysis="18.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-34" weight="240.66424494032" dfnumber="528" searchkey="Frit F34" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.514790" analysis="12.000"/>
<oxide symbol="Na2O" formula="0.485210" analysis="12.500"/>
<oxide symbol="B2O3" formula="0.950900" analysis="27.500"/>
<oxide symbol="SiO2" formula="1.922110" analysis="48.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-38" weight="306.99505132949" dfnumber="530" searchkey="Frit F38" type="16" property1="0">
<chemistry>
<oxide symbol="SrO" formula="0.497830" analysis="16.800"/>
<oxide symbol="ZrO2" formula="0.029897" analysis="1.200"/>
<oxide symbol="B2O3" formula="0.661627" analysis="15.000"/>
<oxide symbol="Al2O3" formula="0.126410" analysis="4.200"/>
<oxide symbol="CaO" formula="0.229836" analysis="4.200"/>
<oxide symbol="SiO2" formula="2.712386" analysis="53.100"/>
<oxide symbol="Na2O" formula="0.272334" analysis="5.500"/>
</chemistry>
</material>
<material name="Fusion Frit F-403" weight="310.62024688519" dfnumber="534" searchkey="Frit F403" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.188808" analysis="6.200"/>
<oxide symbol="BaO" formula="0.709179" analysis="35.000"/>
<oxide symbol="SiO2" formula="2.532511" analysis="49.000"/>
<oxide symbol="CaO" formula="0.265771" analysis="4.800"/>
<oxide symbol="Na2O" formula="0.025050" analysis="0.500"/>
<oxide symbol="ZrO2" formula="0.075626" analysis="3.000"/>
<oxide symbol="B2O3" formula="0.066944" analysis="1.500"/>
</chemistry>
</material>
<material name="Fusion Frit F-493" weight="123.2761929165" dfnumber="538" searchkey="Frit F493" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.076141" analysis="6.300"/>
<oxide symbol="SiO2" formula="1.062514" analysis="51.800"/>
<oxide symbol="K2O" formula="0.078520" analysis="6.000"/>
<oxide symbol="Li2O" formula="0.455046" analysis="11.000"/>
<oxide symbol="Na2O" formula="0.232634" analysis="11.700"/>
<oxide symbol="B2O3" formula="0.233800" analysis="13.200"/>
</chemistry>
</material>
<material name="Fusion Frit F-524" weight="359.19418439658" dfnumber="2402" searchkey="Frit F524" type="16" property1="0">
<chemistry>
<oxide symbol="BaO" formula="0.042260" analysis="1.800"/>
<oxide symbol="SrO" formula="0.277926" analysis="8.000"/>
<oxide symbol="Al2O3" formula="0.317571" analysis="9.000"/>
<oxide symbol="K2O" formula="0.114622" analysis="3.000"/>
<oxide symbol="B2O3" formula="0.620541" analysis="12.000"/>
<oxide symbol="Na2O" formula="0.116101" analysis="2.000"/>
<oxide symbol="SiO2" formula="3.413494" analysis="57.000"/>
<oxide symbol="CaO" formula="0.449091" analysis="7.000"/>
</chemistry>
</material>
<material name="Fusion Frit F-60" weight="266.22273249139" dfnumber="545" searchkey="F60 Fusion, Frit F60" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="2.480611" analysis="56.000"/>
<oxide symbol="CaO" formula="0.355913" analysis="7.500"/>
<oxide symbol="Na2O" formula="0.644087" analysis="15.000"/>
<oxide symbol="B2O3" formula="0.822383" analysis="21.500"/>
</chemistry>
</material>
<material name="Fusion Frit F-69" weight="317.32283464567" dfnumber="547" searchkey="F69 Frit, Frit G69" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.203630" analysis="3.600"/>
<oxide symbol="MgO" formula="1.000000" analysis="12.700"/>
<oxide symbol="B2O3" formula="1.322178" analysis="29.000"/>
<oxide symbol="Al2O3" formula="0.407542" analysis="13.100"/>
<oxide symbol="SiO2" formula="2.196444" analysis="41.600"/>
</chemistry>
</material>
<material name="Fusion Frit F-75" weight="260.99494472829" dfnumber="550" searchkey="F75 Fusion,Frit F75" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="3.039875" analysis="70.000"/>
<oxide symbol="CaO" formula="0.297748" analysis="6.400"/>
<oxide symbol="K2O" formula="0.058184" analysis="2.100"/>
<oxide symbol="Na2O" formula="0.644068" analysis="15.300"/>
<oxide symbol="B2O3" formula="0.093748" analysis="2.500"/>
<oxide symbol="Al2O3" formula="0.094675" analysis="3.700"/>
</chemistry>
</material>
<material name="Fusion Frit F644" weight="210.66938498131" dfnumber="2579" searchkey="Frit F644" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="29.430"/>
<oxide symbol="Al2O3" formula="0.122684" analysis="5.940"/>
<oxide symbol="SiO2" formula="2.265485" analysis="64.630"/>
</chemistry>
</material>
<material name="Fusion Frit FZ-14" weight="235.26253991849" dfnumber="584" searchkey="Frit FZ14" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.169010" analysis="5.000"/>
<oxide symbol="Al2O3" formula="0.320603" analysis="13.900"/>
<oxide symbol="CaO" formula="0.268392" analysis="6.400"/>
<oxide symbol="SiO2" formula="2.023806" analysis="51.700"/>
<oxide symbol="K2O" formula="0.092407" analysis="3.700"/>
<oxide symbol="Na2O" formula="0.341510" analysis="9.000"/>
<oxide symbol="ZnO" formula="0.297691" analysis="10.300"/>
</chemistry>
</material>
<material name="Fusion Frit FZ-16" weight="239.8674566483" dfnumber="556" searchkey="Frit FZ16" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.624394" analysis="40.700"/>
<oxide symbol="CaO" formula="0.179580" analysis="4.200"/>
<oxide symbol="Na2O" formula="0.363670" analysis="9.400"/>
<oxide symbol="ZnO" formula="0.456750" analysis="15.500"/>
<oxide symbol="B2O3" formula="1.040804" analysis="30.200"/>
</chemistry>
</material>
<material name="Fusion Frit FZ-25" weight="320.58086222991" dfnumber="591" searchkey="Frit FZ25" type="16" property1="0">
<chemistry>
<oxide symbol="ZnO" formula="0.027568" analysis="0.700"/>
<oxide symbol="B2O3" formula="0.778422" analysis="16.900"/>
<oxide symbol="Al2O3" formula="0.380297" analysis="12.100"/>
<oxide symbol="CaO" formula="0.028572" analysis="0.500"/>
<oxide symbol="SiO2" formula="2.651060" analysis="49.700"/>
<oxide symbol="K2O" formula="0.183772" analysis="5.400"/>
<oxide symbol="Na2O" formula="0.760087" analysis="14.700"/>
</chemistry>
</material>
<material name="Fusion Frit FZ-376A" weight="1342.1052631579" dfnumber="597" searchkey="Frit FZ376A" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="7.600"/>
<oxide symbol="K2O" formula="0.398927" analysis="2.800"/>
<oxide symbol="SiO2" formula="12.550136" analysis="56.200"/>
<oxide symbol="Na2O" formula="0.995756" analysis="4.600"/>
<oxide symbol="ZnO" formula="0.181366" analysis="1.100"/>
<oxide symbol="ZrO2" formula="0.925815" analysis="8.500"/>
<oxide symbol="B2O3" formula="2.545372" analysis="13.200"/>
<oxide symbol="CaO" formula="1.435407" analysis="6.000"/>
</chemistry>
</material>
<material name="G-200 EU Feldspar" weight="617.85367027613" dfnumber="3175" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="7.055566" analysis="68.500"/>
<oxide symbol="CaO" formula="0.055173" analysis="0.500"/>
<oxide symbol="Al2O3" formula="1.031726" analysis="17.000"/>
<oxide symbol="MgO" formula="0.012289" analysis="0.080"/>
<oxide symbol="Fe2O3" formula="0.003869" analysis="0.100"/>
<oxide symbol="TiO2" formula="0.002324" analysis="0.030"/>
<oxide symbol="K2O" formula="0.722866" analysis="11.000"/>
<oxide symbol="Na2O" formula="0.209673" analysis="2.100"/>
</chemistry>
</material>
<material name="G-200 Feldspar" weight="553.86801473057" dfnumber="800" searchkey="G200 Feldspar, G200 Spar, G 200 Spar, G 200, G 200 Feldspar" type="13" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.636410" analysis="10.800"/>
<oxide symbol="MgO" formula="0.006887" analysis="0.050"/>
<oxide symbol="Fe2O3" formula="0.002775" analysis="0.080"/>
<oxide symbol="CaO" formula="0.079157" analysis="0.800"/>
<oxide symbol="SiO2" formula="6.123550" analysis="66.300"/>
<oxide symbol="Al2O3" formula="1.006783" analysis="18.500"/>
<oxide symbol="Na2O" formula="0.277546" analysis="3.100"/>
</chemistry>
</material>
<material name="G200 HP Feldspar" weight="585.79081690427" dfnumber="3054" searchkey="G200HP Feldspar" type="13" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.051610" analysis="18.300"/>
<oxide symbol="CaO" formula="0.031345" analysis="0.300"/>
<oxide symbol="Fe2O3" formula="0.003297" analysis="0.090"/>
<oxide symbol="K2O" formula="0.883570" analysis="14.200"/>
<oxide symbol="Na2O" formula="0.085085" analysis="0.900"/>
<oxide symbol="SiO2" formula="6.436845" analysis="66.000"/>
</chemistry>
</material>
<material name="Gary Adkins Ohio Clay" weight="369.66956578812" dfnumber="2558" searchkey="" type="" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.152470" analysis="4.380"/>
<oxide symbol="SiO2" formula="3.120919" analysis="57.200"/>
<oxide symbol="TiO2" formula="0.041041" analysis="1.000"/>
<oxide symbol="Al2O3" formula="0.536880" analysis="16.700"/>
<oxide symbol="P2O5" formula="0.020798" analysis="0.900"/>
<oxide symbol="CaO" formula="0.415008" analysis="7.100"/>
<oxide symbol="MnO" formula="0.004625" analysis="0.100"/>
<oxide symbol="Fe2O3" formula="0.143463" analysis="7.000"/>
<oxide symbol="Na2O" formula="0.021156" analysis="0.400"/>
<oxide symbol="MgO" formula="0.390568" analysis="4.800"/>
<oxide symbol="ZrO2" formula="0.000532" analysis="0.020"/>
</chemistry>
</material>
<material name="General Frit GF-106" weight="344.22205864989" dfnumber="610" searchkey="Frit 106, Frit GF106, GF 106, GC 106,Frit GF-106" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="4.379810" analysis="76.470"/>
<oxide symbol="CaO" formula="0.020248" analysis="0.330"/>
<oxide symbol="MgO" formula="0.059790" analysis="0.700"/>
<oxide symbol="Na2O" formula="0.919961" analysis="16.570"/>
<oxide symbol="Al2O3" formula="0.200121" analysis="5.930"/>
</chemistry>
</material>
<material name="General Frit GF-111" weight="191.17607306117" dfnumber="613" searchkey="Frit 111, Frit GF111" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.682986" analysis="20.040"/>
<oxide symbol="Na2O" formula="0.317014" analysis="10.280"/>
<oxide symbol="B2O3" formula="0.640064" analysis="23.300"/>
<oxide symbol="SiO2" formula="1.475162" analysis="46.370"/>
</chemistry>
</material>
<material name="General Frit GF-113" weight="274.77738889013" dfnumber="615" searchkey="Frit 113, Frit GF113" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="2.479149" analysis="54.230"/>
<oxide symbol="CaO" formula="0.690058" analysis="14.090"/>
<oxide symbol="K2O" formula="0.020125" analysis="0.690"/>
<oxide symbol="Na2O" formula="0.289817" analysis="6.540"/>
<oxide symbol="B2O3" formula="0.570027" analysis="14.440"/>
<oxide symbol="Al2O3" formula="0.269901" analysis="10.020"/>
</chemistry>
</material>
<material name="General Frit GF-115" weight="333.65469013051" dfnumber="617" searchkey="Frit 115, Frit GF115" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.679799" analysis="11.430"/>
<oxide symbol="Na2O" formula="0.320201" analysis="5.950"/>
<oxide symbol="B2O3" formula="1.109785" analysis="23.150"/>
<oxide symbol="Al2O3" formula="0.389918" analysis="11.920"/>
<oxide symbol="SiO2" formula="2.639814" analysis="47.550"/>
</chemistry>
</material>
<material name="General Frit GF-134" weight="262.50097647008" dfnumber="623" searchkey="Frit 134, Frit GF134" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="3.061216" analysis="70.080"/>
<oxide symbol="CaO" formula="0.292945" analysis="6.260"/>
<oxide symbol="K2O" formula="0.060476" analysis="2.170"/>
<oxide symbol="Na2O" formula="0.646579" analysis="15.270"/>
<oxide symbol="B2O3" formula="0.101088" analysis="2.680"/>
<oxide symbol="Al2O3" formula="0.090855" analysis="3.530"/>
</chemistry>
</material>
<material name="Gerstley Borate" weight="199.43277312223" dfnumber="806" searchkey="Colemanite, Calcium Borate, Borocalcite" type="15" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.004986" analysis="0.400"/>
<oxide symbol="MgO" formula="0.173205" analysis="3.500"/>
<oxide symbol="P2O5" formula="0.001405" analysis="0.100"/>
<oxide symbol="Na2O" formula="0.128666" analysis="4.000"/>
<oxide symbol="TiO2" formula="0.002496" analysis="0.100"/>
<oxide symbol="B2O3" formula="0.767931" analysis="26.800"/>
<oxide symbol="Al2O3" formula="0.019552" analysis="1.000"/>
<oxide symbol="CaO" formula="0.689661" analysis="19.400"/>
<oxide symbol="SiO2" formula="0.491116" analysis="14.800"/>
<oxide symbol="K2O" formula="0.008468" analysis="0.400"/>
</chemistry>
</material>
<material name="Gillespie Borate" weight="174.90438112948" dfnumber="2141" searchkey="Gilespie Borate" type="" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.106322" analysis="3.770"/>
<oxide symbol="SrO" formula="0.007595" analysis="0.450"/>
<oxide symbol="Al2O3" formula="0.029142" analysis="1.700"/>
<oxide symbol="B2O3" formula="0.615505" analysis="24.500"/>
<oxide symbol="CaO" formula="0.716869" analysis="23.000"/>
<oxide symbol="SiO2" formula="0.343307" analysis="11.800"/>
<oxide symbol="MgO" formula="0.169213" analysis="3.900"/>
</chemistry>
</material>
<material name="GK 129 Bentonite" weight="662.26742504579" dfnumber="808" searchkey="GK129" type="9" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.278823" analysis="2.610"/>
<oxide symbol="TiO2" formula="0.013263" analysis="0.160"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="15.400"/>
<oxide symbol="CaO" formula="0.230224" analysis="1.950"/>
<oxide symbol="SiO2" formula="7.501718" analysis="68.070"/>
<oxide symbol="K2O" formula="0.068202" analysis="0.970"/>
<oxide symbol="Fe2O3" formula="0.078239" analysis="1.890"/>
<oxide symbol="MgO" formula="0.532500" analysis="3.240"/>
</chemistry>
</material>
<material name="Glacier 200 Talc" weight="128.19403492856" dfnumber="809" searchkey="Cyprus Glacier 200 Talc" type="15" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.045702" analysis="2.000"/>
<oxide symbol="MgO" formula="0.954298" analysis="30.000"/>
<oxide symbol="Al2O3" formula="0.006284" analysis="0.500"/>
<oxide symbol="SiO2" formula="1.279807" analysis="60.000"/>
<oxide symbol="Fe2O3" formula="0.008012" analysis="1.000"/>
</chemistry>
</material>
<material name="Glass Cullet" weight="206.89627622453" dfnumber="810" searchkey="Powdered Glass, Cullet" type="15" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.373187" analysis="10.120"/>
<oxide symbol="Fe2O3" formula="0.002974" analysis="0.230"/>
<oxide symbol="K2O" formula="0.001977" analysis="0.090"/>
<oxide symbol="MgO" formula="0.168375" analysis="3.280"/>
<oxide symbol="Na2O" formula="0.456461" analysis="13.680"/>
<oxide symbol="Al2O3" formula="0.023121" analysis="1.140"/>
<oxide symbol="SiO2" formula="2.460133" analysis="71.470"/>
</chemistry>
</material>
<material name="Gleason Ball Clay" weight="389.13791731636" dfnumber="821" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="MnO" formula="0.000547" analysis="0.010"/>
<oxide symbol="TiO2" formula="0.071894" analysis="1.480"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="26.280"/>
<oxide symbol="CaO" formula="0.006227" analysis="0.090"/>
<oxide symbol="P2O5" formula="0.003009" analysis="0.110"/>
<oxide symbol="K2O" formula="0.013185" analysis="0.320"/>
<oxide symbol="SiO2" formula="3.797324" analysis="58.800"/>
<oxide symbol="MgO" formula="0.003852" analysis="0.040"/>
<oxide symbol="Fe2O3" formula="0.034204" analysis="1.410"/>
<oxide symbol="Na2O" formula="0.004382" analysis="0.070"/>
</chemistry>
</material>
<material name="Glomax LL Calcined Kaolin" weight="229.752790333" dfnumber="822" searchkey="Glomax Kaolin, Ajax Glomax Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.006030" analysis="0.420"/>
<oxide symbol="K2O" formula="0.009999" analysis="0.410"/>
<oxide symbol="Na2O" formula="0.011116" analysis="0.300"/>
<oxide symbol="TiO2" formula="0.027027" analysis="0.940"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="44.400"/>
<oxide symbol="SiO2" formula="2.032019" analysis="53.160"/>
</chemistry>
</material>
<material name="Goldart" weight="353.77314814815" dfnumber="198" searchkey="Cedar Heights Goldart" type="9" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.030990" analysis="1.400"/>
<oxide symbol="MgO" formula="0.035153" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.011425" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.079787" analysis="1.800"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="28.800"/>
<oxide symbol="CaO" formula="0.012626" analysis="0.200"/>
<oxide symbol="SiO2" formula="3.252912" analysis="55.200"/>
<oxide symbol="K2O" formula="0.071435" analysis="1.900"/>
</chemistry>
</material>
<material name="Grolleg Kaolin" weight="276.11430045798" dfnumber="831" searchkey="Grolleg China Clay" type="18" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.001035" analysis="0.030"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.000"/>
<oxide symbol="CaO" formula="0.004914" analysis="0.100"/>
<oxide symbol="SiO2" formula="2.201736" analysis="48.000"/>
<oxide symbol="K2O" formula="0.055603" analysis="1.900"/>
<oxide symbol="Fe2O3" formula="0.012061" analysis="0.700"/>
<oxide symbol="MgO" formula="0.020522" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.004446" analysis="0.100"/>
</chemistry>
</material>
<material name="Gunheath Kaolin" weight="263.36173508908" dfnumber="833" searchkey="" type="18" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.041937" analysis="1.500"/>
<oxide symbol="MgO" formula="0.007189" analysis="0.110"/>
<oxide symbol="TiO2" formula="0.002967" analysis="0.090"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.730"/>
<oxide symbol="SiO2" formula="2.052118" analysis="46.830"/>
<oxide symbol="CaO" formula="0.008920" analysis="0.190"/>
<oxide symbol="Fe2O3" formula="0.010041" analysis="0.610"/>
</chemistry>
</material>
<material name="Hardwood Ash" weight="85.292657314058" dfnumber="837" searchkey="Hard wood ash" type="15" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="0.009508" analysis="0.670"/>
<oxide symbol="CaO" formula="0.327031" analysis="21.510"/>
<oxide symbol="Fe2O3" formula="0.003092" analysis="0.580"/>
<oxide symbol="K2O" formula="0.302780" analysis="33.440"/>
<oxide symbol="MnO" formula="0.031278" analysis="2.600"/>
<oxide symbol="MgO" formula="0.335456" analysis="15.850"/>
<oxide symbol="Na2O" formula="0.031641" analysis="2.300"/>
<oxide symbol="P2O5" formula="0.098216" analysis="16.340"/>
</chemistry>
</material>
<material name="Hawthorne Bond" weight="289.457756917" dfnumber="839" searchkey="Hawthorne Fireclay, Hawthorn, HAWTHORN 35m" type="9" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.050333" analysis="0.700"/>
<oxide symbol="Na2O" formula="0.004674" analysis="0.100"/>
<oxide symbol="TiO2" formula="0.068907" analysis="1.900"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="35.200"/>
<oxide symbol="CaO" formula="0.015496" analysis="0.300"/>
<oxide symbol="SiO2" formula="2.458970" analysis="51.000"/>
<oxide symbol="K2O" formula="0.039990" analysis="1.300"/>
<oxide symbol="Fe2O3" formula="0.025355" analysis="1.400"/>
</chemistry>
</material>
<material name="Hectalite 200" weight="142.90254516925" dfnumber="843" searchkey="Hectalite" type="9" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.317124" analysis="60.800"/>
<oxide symbol="CaO" formula="0.280815" analysis="12.100"/>
<oxide symbol="Fe2O3" formula="0.010009" analysis="1.230"/>
<oxide symbol="K2O" formula="0.004561" analysis="0.330"/>
<oxide symbol="Li2O" formula="0.056360" analysis="1.290"/>
<oxide symbol="MgO" formula="0.655826" analysis="20.300"/>
<oxide symbol="Na2O" formula="0.058798" analysis="2.800"/>
<oxide symbol="Al2O3" formula="0.020168" analysis="1.580"/>
</chemistry>
</material>
<material name="Helmer Kaolin" weight="280.06837212875" dfnumber="845" searchkey="Helmar Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.018280" analysis="0.260"/>
<oxide symbol="Na2O" formula="0.003656" analysis="0.080"/>
<oxide symbol="TiO2" formula="0.040071" analysis="1.130"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="36.000"/>
<oxide symbol="CaO" formula="0.024242" analysis="0.480"/>
<oxide symbol="SiO2" formula="2.168608" analysis="46.000"/>
<oxide symbol="K2O" formula="0.015941" analysis="0.530"/>
<oxide symbol="Fe2O3" formula="0.023021" analysis="1.300"/>
</chemistry>
</material>
<material name="Hommel Frit 13" weight="226.6081871345" dfnumber="322" searchkey="" type="16,19" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="0.409855" analysis="10.870"/>
<oxide symbol="Na2O" formula="0.300073" analysis="8.210"/>
<oxide symbol="PbO" formula="0.699927" analysis="68.940"/>
<oxide symbol="B2O3" formula="0.390053" analysis="11.980"/>
</chemistry>
</material>
<material name="Hommel Frit 14" weight="190.94010222437" dfnumber="323" searchkey="" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.680033" analysis="20.000"/>
<oxide symbol="Na2O" formula="0.319967" analysis="10.400"/>
<oxide symbol="B2O3" formula="0.638572" analysis="23.300"/>
<oxide symbol="SiO2" formula="1.472674" analysis="46.400"/>
</chemistry>
</material>
<material name="Hommel Frit 22" weight="385.99953574702" dfnumber="331" searchkey="" type="16,19" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.469942" analysis="6.830"/>
<oxide symbol="PbO" formula="0.530058" analysis="30.650"/>
<oxide symbol="B2O3" formula="0.979973" analysis="17.670"/>
<oxide symbol="SiO2" formula="2.880546" analysis="44.850"/>
</chemistry>
</material>
<material name="Hommel Frit 240" weight="271.16996719718" dfnumber="337" searchkey="" type="16,19" property1="0">
<chemistry>
<oxide symbol="PbO" formula="0.720083" analysis="59.270"/>
<oxide symbol="B2O3" formula="0.560262" analysis="14.380"/>
<oxide symbol="SiO2" formula="0.900140" analysis="19.950"/>
<oxide symbol="Na2O" formula="0.279917" analysis="6.400"/>
</chemistry>
</material>
<material name="Hommel Frit 266" weight="245.92267668401" dfnumber="340" searchkey="" type="16" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.319941" analysis="13.270"/>
<oxide symbol="SiO2" formula="1.310224" analysis="32.020"/>
<oxide symbol="CaO" formula="0.679904" analysis="15.510"/>
<oxide symbol="Na2O" formula="0.320096" analysis="8.070"/>
<oxide symbol="B2O3" formula="1.099939" analysis="31.130"/>
</chemistry>
</material>
<material name="Hommel Frit 267" weight="301.93979877834" dfnumber="341" searchkey="" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.239738" analysis="28.580"/>
<oxide symbol="Al2O3" formula="0.290070" analysis="9.800"/>
<oxide symbol="SiO2" formula="2.049569" analysis="40.800"/>
<oxide symbol="CaO" formula="0.559690" analysis="10.400"/>
<oxide symbol="K2O" formula="0.130122" analysis="4.060"/>
<oxide symbol="Na2O" formula="0.310188" analysis="6.370"/>
</chemistry>
</material>
<material name="Hommel Frit 285" weight="315.55470068661" dfnumber="344" searchkey="" type="16" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.939863" analysis="20.730"/>
<oxide symbol="Al2O3" formula="0.210060" analysis="6.790"/>
<oxide symbol="SiO2" formula="2.720281" analysis="51.810"/>
<oxide symbol="K2O" formula="0.100160" analysis="2.990"/>
<oxide symbol="Na2O" formula="0.899840" analysis="17.680"/>
</chemistry>
</material>
<material name="Hyplas 64 Ball Clay" weight="425" dfnumber="2309" searchkey="Hy Plas 64" type="7" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.085106" analysis="1.600"/>
<oxide symbol="Na2O" formula="0.034274" analysis="0.500"/>
<oxide symbol="K2O" formula="0.108280" analysis="2.400"/>
<oxide symbol="Fe2O3" formula="0.026563" analysis="1.000"/>
<oxide symbol="MgO" formula="0.042184" analysis="0.400"/>
<oxide symbol="SiO2" formula="4.455075" analysis="63.000"/>
<oxide symbol="CaO" formula="0.015152" analysis="0.200"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="24.000"/>
</chemistry>
</material>
<material name="Imco 400 Fireclay" weight="296.61236798441" dfnumber="864" searchkey="" type="14" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="2.447084" analysis="49.600"/>
<oxide symbol="CaO" formula="0.002114" analysis="0.040"/>
<oxide symbol="Fe2O3" formula="0.047627" analysis="2.570"/>
<oxide symbol="K2O" formula="0.034625" analysis="1.100"/>
<oxide symbol="MgO" formula="0.041203" analysis="0.560"/>
<oxide symbol="Na2O" formula="0.002869" analysis="0.060"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="34.400"/>
</chemistry>
</material>
<material name="IMCO Borate" weight="195.4790056138" dfnumber="2167" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.003994" analysis="0.300"/>
<oxide symbol="CaO" formula="0.729013" analysis="19.200"/>
<oxide symbol="SrO" formula="0.041121" analysis="2.000"/>
<oxide symbol="B2O3" formula="0.746753" analysis="24.400"/>
<oxide symbol="Al2O3" formula="0.008353" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.103069" analysis="3.000"/>
<oxide symbol="SiO2" formula="0.747833" analysis="21.100"/>
<oxide symbol="MgO" formula="0.095140" analysis="1.800"/>
<oxide symbol="K2O" formula="0.031657" analysis="1.400"/>
</chemistry>
</material>
<material name="Iron Oxide Black" weight="252.09161980524" dfnumber="873" searchkey="Fe3O4, Black Iron Oxide, BIO, Magnetite Powder, Iron(II,III) Oxide" type="10,17" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="1.000000" analysis="63.400"/>
<oxide symbol="FeO" formula="0.879270" analysis="28.500"/>
</chemistry>
</material>
<material name="Iron Oxide Red" weight="168.42105263158" dfnumber="874" searchkey="Ferric Oxide, Red Iron Oxide, RIO, Iron(III) oxide, Fe2O3, Hematite" type="10,17" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="1.000000" analysis="95.000"/>
</chemistry>
</material>
<material name="Jackson Ball Clay" weight="338.88299726348" dfnumber="906" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.012041" analysis="0.200"/>
<oxide symbol="SiO2" formula="3.062776" analysis="54.500"/>
<oxide symbol="K2O" formula="0.032269" analysis="0.900"/>
<oxide symbol="Fe2O3" formula="0.016887" analysis="0.800"/>
<oxide symbol="MgO" formula="0.025143" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.010895" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.105678" analysis="2.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="30.200"/>
</chemistry>
</material>
<material name="Jasper Slip" weight="428.01981037226" dfnumber="909" searchkey="" type="9" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.027614" analysis="0.400"/>
<oxide symbol="TiO2" formula="0.042856" analysis="0.800"/>
<oxide symbol="Al2O3" formula="0.591674" analysis="14.100"/>
<oxide symbol="CaO" formula="0.541701" analysis="7.100"/>
<oxide symbol="SiO2" formula="3.924108" analysis="55.100"/>
<oxide symbol="K2O" formula="0.122681" analysis="2.700"/>
<oxide symbol="Fe2O3" formula="0.149807" analysis="5.600"/>
<oxide symbol="MgO" formula="0.308004" analysis="2.900"/>
</chemistry>
</material>
<material name="Jordan Fireclay" weight="505.3967202281" dfnumber="912" searchkey="Maryland Ball/Stoneware Clay" type="9,14" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.018020" analysis="0.200"/>
<oxide symbol="SiO2" formula="5.654154" analysis="67.230"/>
<oxide symbol="K2O" formula="0.106778" analysis="1.990"/>
<oxide symbol="Fe2O3" formula="0.054020" analysis="1.710"/>
<oxide symbol="MgO" formula="0.062711" analysis="0.500"/>
<oxide symbol="Na2O" formula="0.016305" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.075913" analysis="1.200"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="20.180"/>
</chemistry>
</material>
<material name="K-200 Feldspar" weight="605.61480769675" dfnumber="914" searchkey="K200 Feldspar" type="13" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.019453" analysis="0.180"/>
<oxide symbol="K2O" formula="0.651980" analysis="10.130"/>
<oxide symbol="Na2O" formula="0.328567" analysis="3.360"/>
<oxide symbol="Al2O3" formula="1.060402" analysis="17.840"/>
<oxide symbol="SiO2" formula="6.858775" analysis="67.990"/>
<oxide symbol="Fe2O3" formula="0.003031" analysis="0.080"/>
</chemistry>
</material>
<material name="K&amp;T Special" weight="372.26277372263" dfnumber="913" searchkey="Kentucky Special Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.012008" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.069887" analysis="1.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="27.400"/>
<oxide symbol="CaO" formula="0.019907" analysis="0.300"/>
<oxide symbol="SiO2" formula="3.301432" analysis="53.300"/>
<oxide symbol="K2O" formula="0.035567" analysis="0.900"/>
<oxide symbol="Fe2O3" formula="0.025593" analysis="1.100"/>
<oxide symbol="MgO" formula="0.046186" analysis="0.500"/>
</chemistry>
</material>
<material name="Kaolin" weight="253.66824173091" dfnumber="925" searchkey="China Clay" type="17,18" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="40.210"/>
<oxide symbol="SiO2" formula="1.996002" analysis="47.290"/>
</chemistry>
</material>
<material name="Kaopaque 20 Kaolin" weight="253.14191533657" dfnumber="928" searchkey="Kaopaque, Kaopaque Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.001256" analysis="0.030"/>
<oxide symbol="TiO2" formula="0.021439" analysis="0.660"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="39.300"/>
<oxide symbol="CaO" formula="0.009715" analysis="0.210"/>
<oxide symbol="SiO2" formula="1.951963" analysis="45.200"/>
<oxide symbol="K2O" formula="0.002204" analysis="0.080"/>
<oxide symbol="Fe2O3" formula="0.005191" analysis="0.320"/>
<oxide symbol="MgO" formula="0.001932" analysis="0.030"/>
</chemistry>
</material>
<material name="Kentucky Stone" weight="517.13670613563" dfnumber="933" searchkey="Kentky Stn, Kentucky Stone Clay" type="7" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.018182" analysis="0.200"/>
<oxide symbol="SiO2" formula="5.855241" analysis="69.000"/>
<oxide symbol="K2O" formula="0.064968" analysis="1.200"/>
<oxide symbol="Fe2O3" formula="0.057375" analysis="1.800"/>
<oxide symbol="MgO" formula="0.063275" analysis="0.500"/>
<oxide symbol="Na2O" formula="0.016452" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.082979" analysis="1.300"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="20.000"/>
</chemistry>
</material>
<material name="Kingman Feldspar" weight="573.2105249863" dfnumber="938" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.052115" analysis="18.720"/>
<oxide symbol="SiO2" formula="6.311670" analysis="66.170"/>
<oxide symbol="Fe2O3" formula="0.003941" analysis="0.110"/>
<oxide symbol="CaO" formula="0.010219" analysis="0.100"/>
<oxide symbol="K2O" formula="0.730886" analysis="12.010"/>
<oxide symbol="Na2O" formula="0.258895" analysis="2.800"/>
</chemistry>
</material>
<material name="KT #1-4 Ball Clay" weight="396.21488066431" dfnumber="943" searchkey="KT1-4, KT#1-4" type="7" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.049051" analysis="0.500"/>
<oxide symbol="Na2O" formula="0.012753" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.094013" analysis="1.900"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="25.800"/>
<oxide symbol="CaO" formula="0.014094" analysis="0.200"/>
<oxide symbol="SiO2" formula="3.979801" analysis="60.500"/>
<oxide symbol="K2O" formula="0.058757" analysis="1.400"/>
<oxide symbol="Fe2O3" formula="0.024709" analysis="1.000"/>
</chemistry>
</material>
<material name="KTS-2 Ball Clay" weight="407.38283530598" dfnumber="946" searchkey="KTS2 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="24.900"/>
<oxide symbol="CaO" formula="0.014604" analysis="0.200"/>
<oxide symbol="SiO2" formula="4.150913" analysis="60.900"/>
<oxide symbol="K2O" formula="0.047835" analysis="1.100"/>
<oxide symbol="Fe2O3" formula="0.025602" analysis="1.000"/>
<oxide symbol="MgO" formula="0.040659" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.013214" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.082030" analysis="1.600"/>
</chemistry>
</material>
<material name="KY Special" weight="370.48128342246" dfnumber="949" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.046018" analysis="0.500"/>
<oxide symbol="TiO2" formula="0.060348" analysis="1.300"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="27.500"/>
<oxide symbol="SiO2" formula="3.363485" analysis="54.500"/>
<oxide symbol="CaO" formula="0.033058" analysis="0.500"/>
<oxide symbol="Fe2O3" formula="0.027818" analysis="1.200"/>
<oxide symbol="K2O" formula="0.043312" analysis="1.100"/>
</chemistry>
</material>
<material name="Kyanite" weight="162.11061665607" dfnumber="951" searchkey="Disthene, Cyanite" type="17,20,24" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.000177" analysis="37.080"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="62.920"/>
</chemistry>
</material>
<material name="Laguna Borate" weight="211.26084492718" dfnumber="2142" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="0.657334" analysis="18.700"/>
<oxide symbol="MgO" formula="0.120571" analysis="2.300"/>
<oxide symbol="Fe2O3" formula="0.001320" analysis="0.100"/>
<oxide symbol="K2O" formula="0.031398" analysis="1.400"/>
<oxide symbol="Na2O" formula="0.136297" analysis="4.000"/>
<oxide symbol="Al2O3" formula="0.167766" analysis="8.100"/>
<oxide symbol="B2O3" formula="0.834723" analysis="27.500"/>
<oxide symbol="CaO" formula="0.711734" analysis="18.900"/>
</chemistry>
</material>
<material name="Lead Bisilicate Frit" weight="343.38461538462" dfnumber="645" searchkey="" type="16,17,19" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="65.000"/>
<oxide symbol="SiO2" formula="1.999744" analysis="35.000"/>
</chemistry>
</material>
<material name="Lead Carbonate" weight="258.00485493007" dfnumber="958" searchkey="White lead" type="15,17" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="86.510"/>
</chemistry>
</material>
<material name="Lepidolite" weight="558.64283909063" dfnumber="963" searchkey="Lithium Mica" type="13,17" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.480225" analysis="26.900"/>
<oxide symbol="SiO2" formula="4.454710" analysis="47.700"/>
<oxide symbol="K2O" formula="0.434958" analysis="7.300"/>
<oxide symbol="Li2O" formula="0.565042" analysis="3.000"/>
</chemistry>
</material>
<material name="Light Magnesium Carbonate" weight="93.503480278422" dfnumber="967" searchkey="Hydrated Magnesium Carbonate Mineral, Hydromagnesite, Magnesium Carbonate Light" type="15,17" property1="0">
<chemistry>
<oxide symbol="MgO" formula="1.000000" analysis="43.090"/>
</chemistry>
</material>
<material name="Limestone" weight="103.65131754312" dfnumber="970" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="P2O5" formula="0.000294" analysis="0.040"/>
<oxide symbol="K2O" formula="0.003653" analysis="0.330"/>
<oxide symbol="SiO2" formula="0.086759" analysis="5.000"/>
<oxide symbol="MgO" formula="0.204170" analysis="7.890"/>
<oxide symbol="Fe2O3" formula="0.003520" analysis="0.540"/>
<oxide symbol="Na2O" formula="0.000841" analysis="0.050"/>
<oxide symbol="TiO2" formula="0.000783" analysis="0.060"/>
<oxide symbol="Al2O3" formula="0.008281" analysis="0.810"/>
<oxide symbol="CaO" formula="0.791336" analysis="42.570"/>
</chemistry>
</material>
<material name="Litharge" weight="223.2" dfnumber="961" searchkey="Lead Oxide, Lead(II) oxide, Yellow lead oxide" type="15,17" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Lithium Carbonate" weight="73.146784486991" dfnumber="975" searchkey="Lith Carb, Li2CO3" type="15,17" property1="0">
<chemistry>
<oxide symbol="Li2O" formula="1.000000" analysis="40.740"/>
</chemistry>
</material>
<material name="Lithospar" weight="612.86863302498" dfnumber="977" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Li2O" formula="0.411321" analysis="2.000"/>
<oxide symbol="Na2O" formula="0.399353" analysis="4.040"/>
<oxide symbol="Al2O3" formula="1.303247" analysis="21.690"/>
<oxide symbol="SiO2" formula="7.072973" analysis="69.360"/>
<oxide symbol="K2O" formula="0.189326" analysis="2.910"/>
</chemistry>
</material>
<material name="M&amp;D Ball Clay" weight="373.21624588364" dfnumber="983" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.046305" analysis="0.500"/>
<oxide symbol="TiO2" formula="0.061191" analysis="1.310"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="27.330"/>
<oxide symbol="SiO2" formula="3.568221" analysis="57.460"/>
<oxide symbol="CaO" formula="0.033263" analysis="0.500"/>
<oxide symbol="Fe2O3" formula="0.053883" analysis="2.310"/>
<oxide symbol="K2O" formula="0.019810" analysis="0.500"/>
</chemistry>
</material>
<material name="Magnesite" weight="84.309623430962" dfnumber="1000" searchkey="Mag Carb, MgCO3, Anhydrous Magnesium Carbonate" type="15,17,24" property1="0">
<chemistry>
<oxide symbol="MgO" formula="1.000000" analysis="47.800"/>
</chemistry>
</material>
<material name="Manganese Carbonate" weight="115.06004543979" dfnumber="1007" searchkey="" type="10,17" property1="0">
<chemistry>
<oxide symbol="MnO" formula="1.000000" analysis="61.620"/>
</chemistry>
</material>
<material name="Manganese Dioxide" weight="86.9" dfnumber="1008" searchkey="Mno2, Pyrolusite, Manganese(IV) oxide" type="10,17" property1="0">
<chemistry>
<oxide symbol="MnO2" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Mastercast Kaolin" weight="263.78356938287" dfnumber="1013" searchkey="" type="18" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.001317" analysis="0.020"/>
<oxide symbol="Na2O" formula="0.000428" analysis="0.010"/>
<oxide symbol="TiO2" formula="0.059114" analysis="1.780"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.440"/>
<oxide symbol="CaO" formula="0.001419" analysis="0.030"/>
<oxide symbol="SiO2" formula="1.994750" analysis="45.180"/>
<oxide symbol="K2O" formula="0.003380" analysis="0.120"/>
<oxide symbol="Fe2O3" formula="0.006302" analysis="0.380"/>
</chemistry>
</material>
<material name="Masterfil Kaolin" weight="268.95874444003" dfnumber="1014" searchkey="" type="18" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.780"/>
<oxide symbol="CaO" formula="0.004813" analysis="0.100"/>
<oxide symbol="SiO2" formula="2.062840" analysis="45.920"/>
<oxide symbol="K2O" formula="0.006305" analysis="0.220"/>
<oxide symbol="Fe2O3" formula="0.011643" analysis="0.690"/>
<oxide symbol="MgO" formula="0.003350" analysis="0.050"/>
<oxide symbol="Na2O" formula="0.000871" analysis="0.020"/>
<oxide symbol="TiO2" formula="0.060147" analysis="1.780"/>
</chemistry>
</material>
<material name="Masterfloat Kaolin" weight="263.78356938287" dfnumber="1015" searchkey="" type="18" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.001317" analysis="0.020"/>
<oxide symbol="Na2O" formula="0.000428" analysis="0.010"/>
<oxide symbol="TiO2" formula="0.059114" analysis="1.780"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.440"/>
<oxide symbol="CaO" formula="0.001419" analysis="0.030"/>
<oxide symbol="SiO2" formula="1.994750" analysis="45.180"/>
<oxide symbol="K2O" formula="0.003380" analysis="0.120"/>
<oxide symbol="Fe2O3" formula="0.006302" analysis="0.380"/>
</chemistry>
</material>
<material name="MC 200K Feldspar" weight="598.89658045941" dfnumber="3059" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.002307" analysis="0.060"/>
<oxide symbol="CaO" formula="0.021931" analysis="0.200"/>
<oxide symbol="K2O" formula="0.839160" analysis="12.850"/>
<oxide symbol="Na2O" formula="0.138909" analysis="1.400"/>
<oxide symbol="Al2O3" formula="1.091619" analysis="18.100"/>
<oxide symbol="SiO2" formula="6.571330" analysis="64.200"/>
</chemistry>
</material>
<material name="Minspar 200" weight="568.06272935284" dfnumber="1031" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.002499" analysis="0.070"/>
<oxide symbol="CaO" formula="0.152700" analysis="1.500"/>
<oxide symbol="K2O" formula="0.248567" analysis="4.100"/>
<oxide symbol="Na2O" formula="0.598732" analysis="6.500"/>
<oxide symbol="Al2O3" formula="1.019019" analysis="18.200"/>
<oxide symbol="SiO2" formula="6.537702" analysis="68.800"/>
</chemistry>
</material>
<material name="Mullite" weight="178.94736842105" dfnumber="1054" searchkey="Mulite" type="5,17,24" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.005772" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.013438" analysis="0.600"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="57.000"/>
<oxide symbol="SiO2" formula="1.220772" analysis="41.000"/>
<oxide symbol="K2O" formula="0.003799" analysis="0.200"/>
<oxide symbol="Fe2O3" formula="0.011184" analysis="1.000"/>
</chemistry>
</material>
<material name="Murrays Borate" weight="186.64176821906" dfnumber="2143" searchkey="Murray Borate" type="" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.968070" analysis="36.100"/>
<oxide symbol="SiO2" formula="0.863335" analysis="27.800"/>
<oxide symbol="CaO" formula="0.828410" analysis="24.900"/>
<oxide symbol="Na2O" formula="0.171590" analysis="5.700"/>
<oxide symbol="Al2O3" formula="0.009149" analysis="0.500"/>
</chemistry>
</material>
<material name="Navajo Pumice" weight="769.48083067093" dfnumber="1067" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="12.520"/>
<oxide symbol="K2O" formula="0.475672" analysis="5.500"/>
<oxide symbol="MgO" formula="0.034367" analysis="0.170"/>
<oxide symbol="SiO2" formula="10.058316" analysis="74.200"/>
<oxide symbol="Fe2O3" formula="0.082488" analysis="1.620"/>
<oxide symbol="CaO" formula="0.063898" analysis="0.440"/>
</chemistry>
</material>
<material name="NC-4 Feldspar" weight="554.6860996634" dfnumber="1068" searchkey="NC4 Feldspar, Spruce Pine #4 Spar" type="13" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="6.320827" analysis="68.150"/>
<oxide symbol="CaO" formula="0.139107" analysis="1.400"/>
<oxide symbol="Fe2O3" formula="0.002439" analysis="0.070"/>
<oxide symbol="K2O" formula="0.242614" analysis="4.100"/>
<oxide symbol="MgO" formula="0.006916" analysis="0.050"/>
<oxide symbol="Na2O" formula="0.611364" analysis="6.800"/>
<oxide symbol="Al2O3" formula="1.030134" analysis="18.850"/>
</chemistry>
</material>
<material name="Nepheline Syenite" weight="437.76824034335" dfnumber="1069" searchkey="Neph Sy" type="13,17" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="23.300"/>
<oxide symbol="SiO2" formula="4.421386" analysis="60.700"/>
<oxide symbol="MgO" formula="0.010863" analysis="0.100"/>
<oxide symbol="CaO" formula="0.054623" analysis="0.700"/>
<oxide symbol="Fe2O3" formula="0.002736" analysis="0.100"/>
<oxide symbol="K2O" formula="0.213772" analysis="4.600"/>
<oxide symbol="Na2O" formula="0.691956" analysis="9.800"/>
</chemistry>
</material>
<material name="Nepheline Syenite A270" weight="440.30787653811" dfnumber="2963" searchkey="Spectrum Nepheline Syenite, Nepheline Syenite Spectrum" type="13" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.019059" analysis="23.600"/>
<oxide symbol="Na2O" formula="0.745907" analysis="10.500"/>
<oxide symbol="K2O" formula="0.224428" analysis="4.800"/>
<oxide symbol="MgO" formula="0.002186" analysis="0.020"/>
<oxide symbol="Fe2O3" formula="0.002202" analysis="0.080"/>
<oxide symbol="CaO" formula="0.027478" analysis="0.350"/>
<oxide symbol="SiO2" formula="4.411734" analysis="60.200"/>
</chemistry>
</material>
<material name="Newman Red Clay" weight="565.43673761514" dfnumber="1071" searchkey="Newman Fireclay" type="9" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.022740" analysis="0.230"/>
<oxide symbol="TiO2" formula="0.157273" analysis="2.050"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="16.640"/>
<oxide symbol="SiO2" formula="6.084931" analysis="59.660"/>
<oxide symbol="Fe2O3" formula="0.213777" analysis="5.580"/>
<oxide symbol="MgO" formula="0.205341" analysis="1.350"/>
</chemistry>
</material>
<material name="Nickel Carbonate" weight="118.70332115048" dfnumber="1073" searchkey="NiCO3" type="10,17" property1="0">
<chemistry>
<oxide symbol="NiO" formula="1.000000" analysis="62.930"/>
</chemistry>
</material>
<material name="No. 5 Ball Clay" weight="357.88778980387" dfnumber="1079" searchkey="OH #5, OH#5, Old Hickory #5 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.016042" analysis="0.180"/>
<oxide symbol="Na2O" formula="0.005214" analysis="0.090"/>
<oxide symbol="TiO2" formula="0.056638" analysis="1.260"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="28.400"/>
<oxide symbol="CaO" formula="0.003841" analysis="0.060"/>
<oxide symbol="SiO2" formula="3.513862" analysis="58.800"/>
<oxide symbol="K2O" formula="0.030501" analysis="0.800"/>
<oxide symbol="Fe2O3" formula="0.017733" analysis="0.790"/>
</chemistry>
</material>
<material name="NP Blend Ball Clay" weight="346.35756449227" dfnumber="1085" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="29.450"/>
<oxide symbol="CaO" formula="0.018460" analysis="0.299"/>
<oxide symbol="SiO2" formula="3.140660" analysis="54.498"/>
<oxide symbol="K2O" formula="0.034856" analysis="0.948"/>
<oxide symbol="Fe2O3" formula="0.024872" analysis="1.149"/>
<oxide symbol="MgO" formula="0.034291" analysis="0.399"/>
<oxide symbol="Na2O" formula="0.013910" analysis="0.249"/>
<oxide symbol="TiO2" formula="0.069357" analysis="1.600"/>
</chemistry>
</material>
<material name="Nytal Talc" weight="111.1241083564" dfnumber="1090" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.006093" analysis="0.340"/>
<oxide symbol="Al2O3" formula="0.003377" analysis="0.310"/>
<oxide symbol="SiO2" formula="1.020533" analysis="55.200"/>
<oxide symbol="Fe2O3" formula="0.001111" analysis="0.160"/>
<oxide symbol="CaO" formula="0.166768" analysis="8.420"/>
<oxide symbol="MnO" formula="0.002664" analysis="0.170"/>
<oxide symbol="MgO" formula="0.827139" analysis="30.000"/>
</chemistry>
</material>
<material name="Oakwood Ash" weight="85.292657314058" dfnumber="1092" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.003092" analysis="0.580"/>
<oxide symbol="K2O" formula="0.302780" analysis="33.440"/>
<oxide symbol="MnO" formula="0.031278" analysis="2.600"/>
<oxide symbol="MgO" formula="0.335456" analysis="15.850"/>
<oxide symbol="Na2O" formula="0.031641" analysis="2.300"/>
<oxide symbol="P2O5" formula="0.098216" analysis="16.340"/>
<oxide symbol="SiO2" formula="0.009508" analysis="0.670"/>
<oxide symbol="CaO" formula="0.327031" analysis="21.510"/>
</chemistry>
</material>
<material name="Old Hickory FC340 Ball Clay" weight="423.23651452282" dfnumber="309" searchkey="FC-340 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.007509" analysis="0.110"/>
<oxide symbol="Fe2O3" formula="0.026717" analysis="1.010"/>
<oxide symbol="TiO2" formula="0.067273" analysis="1.270"/>
<oxide symbol="CaO" formula="0.003772" analysis="0.050"/>
<oxide symbol="MgO" formula="0.031506" analysis="0.300"/>
<oxide symbol="SiO2" formula="4.368984" analysis="62.040"/>
<oxide symbol="K2O" formula="0.053017" analysis="1.180"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="24.100"/>
</chemistry>
</material>
<material name="Old Hickory No. 1 Glaze Ball Clay" weight="351.72413793103" dfnumber="1078" searchkey="Glaze #1" type="7" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="29.000"/>
<oxide symbol="CaO" formula="0.006270" analysis="0.100"/>
<oxide symbol="SiO2" formula="3.447014" analysis="58.900"/>
<oxide symbol="K2O" formula="0.022403" analysis="0.600"/>
<oxide symbol="Fe2O3" formula="0.019784" analysis="0.900"/>
<oxide symbol="MgO" formula="0.017455" analysis="0.200"/>
<oxide symbol="Na2O" formula="0.005673" analysis="0.100"/>
<oxide symbol="TiO2" formula="0.044021" analysis="1.000"/>
</chemistry>
</material>
<material name="OM #4 Ball Clay" weight="390.39829630965" dfnumber="1098" searchkey="OM4 Ball Clay, OM4, OM#4, OM 4, Old Mine #4, OM-4 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.012511" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.097080" analysis="2.000"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="26.300"/>
<oxide symbol="CaO" formula="0.013826" analysis="0.200"/>
<oxide symbol="SiO2" formula="3.852515" analysis="59.700"/>
<oxide symbol="K2O" formula="0.045288" analysis="1.100"/>
<oxide symbol="Fe2O3" formula="0.031511" analysis="1.300"/>
<oxide symbol="MgO" formula="0.048118" analysis="0.500"/>
</chemistry>
</material>
<material name="optiKast Kaolin" weight="263.47430133335" dfnumber="3115" searchkey="OptiCast" type="18" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.008236" analysis="0.500"/>
<oxide symbol="TiO2" formula="0.052779" analysis="1.600"/>
<oxide symbol="CaO" formula="0.004698" analysis="0.100"/>
<oxide symbol="K2O" formula="0.002798" analysis="0.100"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.700"/>
<oxide symbol="Na2O" formula="0.004251" analysis="0.100"/>
<oxide symbol="SiO2" formula="1.982226" analysis="45.200"/>
</chemistry>
</material>
<material name="Oxford Feldspar" weight="688.41154851939" dfnumber="1103" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.588692" analysis="8.070"/>
<oxide symbol="Na2O" formula="0.363536" analysis="3.280"/>
<oxide symbol="Al2O3" formula="1.168867" analysis="17.350"/>
<oxide symbol="SiO2" formula="8.097429" analysis="70.820"/>
<oxide symbol="Fe2O3" formula="0.003865" analysis="0.090"/>
<oxide symbol="CaO" formula="0.047771" analysis="0.390"/>
</chemistry>
</material>
<material name="Pearl Ash Calcined" weight="94.2" dfnumber="1111" searchkey="Potash Calcined, Calcined Potash" type="15,17" property1="0">
<chemistry>
<oxide symbol="K2O" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Pemco Frit P-25" weight="326.35131775005" dfnumber="671" searchkey="Pemco 25, Pemco Frit 25" type="16" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.760087" analysis="14.700"/>
<oxide symbol="ZnO" formula="0.027568" analysis="0.700"/>
<oxide symbol="B2O3" formula="0.778422" analysis="16.900"/>
<oxide symbol="Al2O3" formula="0.380297" analysis="12.100"/>
<oxide symbol="CaO" formula="0.028572" analysis="0.500"/>
<oxide symbol="SiO2" formula="2.651060" analysis="49.700"/>
<oxide symbol="K2O" formula="0.183772" analysis="5.400"/>
<oxide symbol="F" formula="0.303708" analysis="1.800"/>
</chemistry>
</material>
<material name="Pemco Frit P-311" weight="275.02250609207" dfnumber="677" searchkey="Frit 311, Frit P311" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="2.484812" analysis="54.300"/>
<oxide symbol="CaO" formula="0.691233" analysis="14.100"/>
<oxide symbol="K2O" formula="0.020437" analysis="0.700"/>
<oxide symbol="Na2O" formula="0.288330" analysis="6.500"/>
<oxide symbol="B2O3" formula="0.569012" analysis="14.400"/>
<oxide symbol="Al2O3" formula="0.269630" analysis="10.000"/>
</chemistry>
</material>
<material name="Pemco Frit P-54" weight="190.7493528715" dfnumber="687" searchkey="Frit 54, Frit P54, Pemco 54" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.680033" analysis="20.000"/>
<oxide symbol="Na2O" formula="0.319967" analysis="10.400"/>
<oxide symbol="B2O3" formula="0.638572" analysis="23.300"/>
<oxide symbol="SiO2" formula="1.469500" analysis="46.300"/>
</chemistry>
</material>
<material name="Pemco Frit P-67" weight="310.24752311556" dfnumber="694" searchkey="Frit 67, Frit P67, Pemco 67" type="16" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.691282" analysis="12.500"/>
<oxide symbol="K2O" formula="0.118566" analysis="3.600"/>
<oxide symbol="Na2O" formula="0.190152" analysis="3.800"/>
<oxide symbol="B2O3" formula="1.158971" analysis="26.000"/>
<oxide symbol="Al2O3" formula="0.368039" analysis="12.100"/>
<oxide symbol="SiO2" formula="2.168119" analysis="42.000"/>
</chemistry>
</material>
<material name="Pemco Frit P-83" weight="342.26829417899" dfnumber="479" searchkey="Frit P83, Frit 83" type="16,19" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="0.260144" analysis="5.290"/>
<oxide symbol="SiO2" formula="2.430617" analysis="42.680"/>
<oxide symbol="Na2O" formula="0.279887" analysis="5.070"/>
<oxide symbol="PbO" formula="0.720113" analysis="46.960"/>
</chemistry>
</material>
<material name="Pemco Frit P-926" weight="225.57487105122" dfnumber="702" searchkey="Frit 926, Frit P926" type="16" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.895429" analysis="50.500"/>
<oxide symbol="CaO" formula="0.683560" analysis="17.000"/>
<oxide symbol="K2O" formula="0.007184" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.309256" analysis="8.500"/>
<oxide symbol="B2O3" formula="0.606070" analysis="18.700"/>
<oxide symbol="Al2O3" formula="0.110576" analysis="5.000"/>
</chemistry>
</material>
<material name="Pemco Frit Pb-316" weight="364.0745187602" dfnumber="352" searchkey="Frit P-316, Pemco 316, Pemco Frit Pb316" type="16,19" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="61.300"/>
<oxide symbol="Al2O3" formula="0.249880" analysis="7.000"/>
<oxide symbol="SiO2" formula="1.919913" analysis="31.690"/>
</chemistry>
</material>
<material name="Petalite" weight="612.53854059609" dfnumber="1114" searchkey="" type="13,17,21" property1="0">
<chemistry>
<oxide symbol="Li2O" formula="1.000000" analysis="4.865"/>
<oxide symbol="Al2O3" formula="0.999879" analysis="16.650"/>
<oxide symbol="SiO2" formula="7.999183" analysis="78.485"/>
</chemistry>
</material>
<material name="Pine Wood Ash" weight="93.861819313577" dfnumber="1119" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.109191" analysis="10.960"/>
<oxide symbol="MnO" formula="0.033621" analysis="2.540"/>
<oxide symbol="MgO" formula="0.191190" analysis="8.210"/>
<oxide symbol="Na2O" formula="0.011655" analysis="0.770"/>
<oxide symbol="P2O5" formula="0.030886" analysis="4.670"/>
<oxide symbol="SiO2" formula="0.031231" analysis="2.000"/>
<oxide symbol="CaO" formula="0.687553" analysis="41.100"/>
<oxide symbol="Fe2O3" formula="0.000411" analysis="0.070"/>
</chemistry>
</material>
<material name="Pioneer 2661 Talc" weight="124.32556555141" dfnumber="1121" searchkey="Pioneer Ceramic Talc, Pioneer Talc, Pioneer 2882" type="15" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.006171" analysis="0.500"/>
<oxide symbol="SiO2" formula="1.120575" analysis="53.500"/>
<oxide symbol="Fe2O3" formula="0.003934" analysis="0.500"/>
<oxide symbol="TiO2" formula="0.001575" analysis="0.100"/>
<oxide symbol="CaO" formula="0.078536" analysis="3.500"/>
<oxide symbol="K2O" formula="0.004009" analysis="0.300"/>
<oxide symbol="MgO" formula="0.921464" analysis="29.500"/>
</chemistry>
</material>
<material name="Pioneer Kaolin" weight="265.8851976068" dfnumber="1120" searchkey="Georgia Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="MgO" formula="0.006608" analysis="0.100"/>
<oxide symbol="SiO2" formula="2.011791" analysis="45.400"/>
<oxide symbol="Na2O" formula="0.004295" analysis="0.100"/>
<oxide symbol="Fe2O3" formula="0.006658" analysis="0.400"/>
<oxide symbol="TiO2" formula="0.046664" analysis="1.400"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.300"/>
<oxide symbol="CaO" formula="0.009494" analysis="0.200"/>
</chemistry>
</material>
<material name="Potash Feldspar" weight="556.73758865248" dfnumber="1135" searchkey="K-Feldspar, Orthoclase, K Feldspar, Potassium Feldspar" type="13,17,21" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.999944" analysis="18.320"/>
<oxide symbol="SiO2" formula="5.999056" analysis="64.760"/>
<oxide symbol="K2O" formula="1.000000" analysis="16.920"/>
</chemistry>
</material>
<material name="PV Clay" weight="803.14960629921" dfnumber="1152" searchkey="Plastic Vitrox, P.V. Clay, P. V. Clay, Plas Vitrox" type="13" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.116586" analysis="0.900"/>
<oxide symbol="TiO2" formula="0.010052" analysis="0.100"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="12.700"/>
<oxide symbol="CaO" formula="0.143164" analysis="1.000"/>
<oxide symbol="SiO2" formula="10.223119" analysis="76.500"/>
<oxide symbol="K2O" formula="0.426300" analysis="5.000"/>
<oxide symbol="Fe2O3" formula="0.025098" analysis="0.500"/>
<oxide symbol="MgO" formula="0.099646" analysis="0.500"/>
</chemistry>
</material>
<material name="Pyrax Pyrophyllite" weight="634.26289604609" dfnumber="1154" searchkey="" type="5" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.011307" analysis="0.100"/>
<oxide symbol="SiO2" formula="8.253657" analysis="78.200"/>
<oxide symbol="K2O" formula="0.121883" analysis="1.810"/>
<oxide symbol="Fe2O3" formula="0.007929" analysis="0.200"/>
<oxide symbol="MgO" formula="0.015740" analysis="0.100"/>
<oxide symbol="Na2O" formula="0.030693" analysis="0.300"/>
<oxide symbol="TiO2" formula="0.007939" analysis="0.100"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="16.080"/>
</chemistry>
</material>
<material name="Pyrofrac" weight="618.18181818182" dfnumber="1158" searchkey="" type="5" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.030948" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.019941" analysis="0.200"/>
<oxide symbol="K2O" formula="0.013125" analysis="0.200"/>
<oxide symbol="Fe2O3" formula="0.038636" analysis="1.000"/>
<oxide symbol="SiO2" formula="7.909847" analysis="76.900"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="16.500"/>
</chemistry>
</material>
<material name="Pyrophyl" weight="456.92852793002" dfnumber="2268" searchkey="" type="5" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.020011" analysis="0.700"/>
<oxide symbol="SiO2" formula="5.578595" analysis="73.300"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="22.300"/>
<oxide symbol="TiO2" formula="0.022899" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.014755" analysis="0.200"/>
<oxide symbol="K2O" formula="0.009711" analysis="0.200"/>
</chemistry>
</material>
<material name="Pyrophyllite" weight="360.42402826855" dfnumber="1167" searchkey="Pyrophillite" type="5,17,20,24" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="28.300"/>
<oxide symbol="SiO2" formula="4.060018" analysis="67.700"/>
</chemistry>
</material>
<material name="Pyrotrol" weight="539.12731073225" dfnumber="2270" searchkey="" type="5" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.017409" analysis="0.200"/>
<oxide symbol="K2O" formula="0.011458" analysis="0.200"/>
<oxide symbol="Fe2O3" formula="0.013492" analysis="0.400"/>
<oxide symbol="SiO2" formula="6.914402" analysis="77.000"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="18.900"/>
<oxide symbol="TiO2" formula="0.027018" analysis="0.400"/>
</chemistry>
</material>
<material name="Ravenscrag Slip" weight="369.29476644747" dfnumber="1178" searchkey="" type="9" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.571456" analysis="8.500"/>
<oxide symbol="SiO2" formula="3.558240" analysis="56.700"/>
<oxide symbol="K2O" formula="0.164157" analysis="4.100"/>
<oxide symbol="Fe2O3" formula="0.025930" analysis="1.100"/>
<oxide symbol="MgO" formula="0.233971" analysis="2.500"/>
<oxide symbol="Na2O" formula="0.030416" analysis="0.500"/>
<oxide symbol="TiO2" formula="0.018882" analysis="0.400"/>
<oxide symbol="Al2O3" formula="0.569439" analysis="15.400"/>
</chemistry>
</material>
<material name="Red Lead" weight="228.52462373298" dfnumber="1186" searchkey="Minium, Lead(II,IV) oxide" type="15,17" property1="0">
<chemistry>
<oxide symbol="PbO" formula="1.000000" analysis="97.670"/>
</chemistry>
</material>
<material name="Redart" weight="657.64023210832" dfnumber="1191" searchkey="Red Art" type="9" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="7.107110" analysis="64.950"/>
<oxide symbol="MgO" formula="0.259466" analysis="1.590"/>
<oxide symbol="Fe2O3" formula="0.289773" analysis="7.050"/>
<oxide symbol="Na2O" formula="0.040307" analysis="0.380"/>
<oxide symbol="TiO2" formula="0.089716" analysis="1.090"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="15.510"/>
<oxide symbol="CaO" formula="0.030479" analysis="0.260"/>
<oxide symbol="P2O5" formula="0.010196" analysis="0.220"/>
<oxide symbol="K2O" formula="0.289725" analysis="4.150"/>
</chemistry>
</material>
<material name="Redearth" weight="695.29652351738" dfnumber="1192" searchkey="Red Earth" type="9" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.166002" analysis="3.820"/>
<oxide symbol="Na2O" formula="0.081866" analysis="0.730"/>
<oxide symbol="MnO" formula="0.001961" analysis="0.020"/>
<oxide symbol="TiO2" formula="0.053953" analysis="0.620"/>
<oxide symbol="BaO" formula="0.010885" analysis="0.240"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="14.670"/>
<oxide symbol="CaO" formula="0.060730" analysis="0.490"/>
<oxide symbol="P2O5" formula="0.015680" analysis="0.320"/>
<oxide symbol="K2O" formula="0.241361" analysis="3.270"/>
<oxide symbol="SiO2" formula="7.981449" analysis="68.990"/>
<oxide symbol="MgO" formula="0.194959" analysis="1.130"/>
</chemistry>
</material>
<material name="Rutile" weight="88.8666444222" dfnumber="1204" searchkey="" type="10,17" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="1.000000" analysis="90.000"/>
<oxide symbol="Fe2O3" formula="0.055486" analysis="10.000"/>
</chemistry>
</material>
<material name="S-3 Ball Clay" weight="424.18911335578" dfnumber="1205" searchkey="s3 ball clay, Hick S-3, Old Hickory S-3 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.049628" analysis="1.100"/>
<oxide symbol="Fe2O3" formula="0.027625" analysis="1.040"/>
<oxide symbol="MgO" formula="0.027419" analysis="0.260"/>
<oxide symbol="Na2O" formula="0.007540" analysis="0.110"/>
<oxide symbol="TiO2" formula="0.063830" analysis="1.200"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="24.000"/>
<oxide symbol="CaO" formula="0.001515" analysis="0.020"/>
<oxide symbol="SiO2" formula="4.327787" analysis="61.200"/>
</chemistry>
</material>
<material name="Sagger XX Ball Clay" weight="349.67432293452" dfnumber="1211" searchkey="XX Sagger, XX Sagger Ball Clay, Saggar" type="7" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.074836" analysis="1.710"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="29.170"/>
<oxide symbol="CaO" formula="0.031165" analysis="0.500"/>
<oxide symbol="SiO2" formula="3.300670" analysis="56.730"/>
<oxide symbol="K2O" formula="0.033037" analysis="0.890"/>
<oxide symbol="Fe2O3" formula="0.015080" analysis="0.690"/>
<oxide symbol="MgO" formula="0.026030" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.016920" analysis="0.300"/>
</chemistry>
</material>
<material name="Seriphyl" weight="638.15586419753" dfnumber="2269" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.270701" analysis="4.000"/>
<oxide symbol="Fe2O3" formula="0.159375" analysis="4.000"/>
<oxide symbol="SiO2" formula="7.690308" analysis="72.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="16.000"/>
<oxide symbol="TiO2" formula="0.031915" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.041129" analysis="0.400"/>
</chemistry>
</material>
<material name="Sil-o-spar" weight="782.49028533237" dfnumber="1244" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="10.099701" analysis="77.370"/>
<oxide symbol="Al2O3" formula="1.036043" analysis="13.470"/>
<oxide symbol="Na2O" formula="0.614971" analysis="4.860"/>
<oxide symbol="K2O" formula="0.238191" analysis="2.860"/>
<oxide symbol="CaO" formula="0.146837" analysis="1.050"/>
<oxide symbol="Fe2O3" formula="0.002942" analysis="0.060"/>
</chemistry>
</material>
<material name="Silica" weight="60.1" dfnumber="1245" searchkey="" type="17,25" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Sledge Ball Clay" weight="419.29180767572" dfnumber="1260" searchkey="" type="7" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="4.393028" analysis="62.969"/>
<oxide symbol="CaO" formula="0.029970" analysis="0.401"/>
<oxide symbol="Fe2O3" formula="0.024004" analysis="0.916"/>
<oxide symbol="K2O" formula="0.017982" analysis="0.404"/>
<oxide symbol="MgO" formula="0.042033" analysis="0.404"/>
<oxide symbol="TiO2" formula="0.094982" analysis="1.810"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="24.327"/>
</chemistry>
</material>
<material name="Snobrite Kaolin" weight="256.73294739492" dfnumber="1262" searchkey="" type="18" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.915031" analysis="44.830"/>
<oxide symbol="Fe2O3" formula="0.012034" analysis="0.750"/>
<oxide symbol="CaO" formula="0.011898" analysis="0.260"/>
<oxide symbol="TiO2" formula="0.016066" analysis="0.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="39.730"/>
</chemistry>
</material>
<material name="Soda Feldspar" weight="524.53468697124" dfnumber="1264" searchkey="Na-Feldspar, Na Feldspar, Albite" type="13,17,21" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="11.820"/>
<oxide symbol="Al2O3" formula="0.999701" analysis="19.440"/>
<oxide symbol="SiO2" formula="5.999420" analysis="68.740"/>
</chemistry>
</material>
<material name="Sodium Carbonate" weight="124" dfnumber="1263" searchkey="Soda Ash, Sodium Caronate Monohydrate, Na2CO3" type="15,17" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="50.000"/>
</chemistry>
</material>
<material name="Sodium Carbonate Decahydrate" weight="285.9778597786" dfnumber="1267" searchkey="Washing Soda, Hydrous Sodium Carbonate" type="11,17" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="1.000000" analysis="21.680"/>
</chemistry>
</material>
<material name="Soft Wood Ash" weight="93.861819313577" dfnumber="1277" searchkey="Softwood Ash" type="15" property1="0">
<chemistry>
<oxide symbol="P2O5" formula="0.030886" analysis="4.670"/>
<oxide symbol="SiO2" formula="0.031231" analysis="2.000"/>
<oxide symbol="CaO" formula="0.687553" analysis="41.100"/>
<oxide symbol="Fe2O3" formula="0.000411" analysis="0.070"/>
<oxide symbol="K2O" formula="0.109191" analysis="10.960"/>
<oxide symbol="MnO" formula="0.033621" analysis="2.540"/>
<oxide symbol="MgO" formula="0.191190" analysis="8.210"/>
<oxide symbol="Na2O" formula="0.011655" analysis="0.770"/>
</chemistry>
</material>
<material name="SP-G Feldspar" weight="557.65186998024" dfnumber="2354" searchkey="" type="13" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.616316" analysis="6.820"/>
<oxide symbol="K2O" formula="0.243862" analysis="4.100"/>
<oxide symbol="CaO" formula="0.139822" analysis="1.400"/>
<oxide symbol="Fe2O3" formula="0.002101" analysis="0.060"/>
<oxide symbol="SiO2" formula="6.353341" analysis="68.150"/>
<oxide symbol="Al2O3" formula="1.039278" analysis="18.920"/>
</chemistry>
</material>
<material name="Spinks Blend Ball" weight="381.32115026435" dfnumber="1284" searchkey="Spinks Blend #1, Spinks Blend Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.027070" analysis="0.670"/>
<oxide symbol="SiO2" formula="3.717312" analysis="58.700"/>
<oxide symbol="MgO" formula="0.022666" analysis="0.240"/>
<oxide symbol="Fe2O3" formula="0.025215" analysis="1.060"/>
<oxide symbol="Na2O" formula="0.011663" analysis="0.190"/>
<oxide symbol="MnO" formula="0.001074" analysis="0.020"/>
<oxide symbol="TiO2" formula="0.071451" analysis="1.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="26.800"/>
<oxide symbol="CaO" formula="0.015604" analysis="0.230"/>
<oxide symbol="P2O5" formula="0.002950" analysis="0.110"/>
</chemistry>
</material>
<material name="Spodumene" weight="372.07215980025" dfnumber="1287" searchkey="" type="13,17" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="3.998292" analysis="64.590"/>
<oxide symbol="Li2O" formula="1.000000" analysis="8.010"/>
<oxide symbol="Al2O3" formula="0.999753" analysis="27.410"/>
</chemistry>
</material>
<material name="Standard Porcelain Kaolin" weight="276.08478341355" dfnumber="1596" searchkey="English Standard Porcelain, Eng Stn Porc, Standard Porcelain China Clay" type="18" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.001035" analysis="0.030"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.000"/>
<oxide symbol="CaO" formula="0.004914" analysis="0.100"/>
<oxide symbol="SiO2" formula="2.201736" analysis="48.000"/>
<oxide symbol="K2O" formula="0.046824" analysis="1.600"/>
<oxide symbol="Fe2O3" formula="0.010338" analysis="0.600"/>
<oxide symbol="MgO" formula="0.020522" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.004446" analysis="0.100"/>
</chemistry>
</material>
<material name="Strontium Carbonate" weight="147.57834757835" dfnumber="1609" searchkey="Strontianite" type="15,17" property1="0">
<chemistry>
<oxide symbol="SrO" formula="1.000000" analysis="70.200"/>
</chemistry>
</material>
<material name="Super Standard Porcelain" weight="273.2807433506" dfnumber="2295" searchkey="Super Standard Porcelain Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="37.320"/>
<oxide symbol="TiO2" formula="0.017103" analysis="0.500"/>
<oxide symbol="K2O" formula="0.049034" analysis="1.690"/>
<oxide symbol="Na2O" formula="0.004408" analysis="0.100"/>
<oxide symbol="MgO" formula="0.013564" analysis="0.200"/>
<oxide symbol="CaO" formula="0.009744" analysis="0.200"/>
<oxide symbol="SiO2" formula="2.141929" analysis="47.100"/>
<oxide symbol="Fe2O3" formula="0.010420" analysis="0.610"/>
</chemistry>
</material>
<material name="Superpax" weight="183.28758767917" dfnumber="2144" searchkey="" type="" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.000000" analysis="32.790"/>
<oxide symbol="ZrO2" formula="0.999737" analysis="67.210"/>
</chemistry>
</material>
<material name="Suzorite 325-PE" weight="122.10827153176" dfnumber="2357" searchkey="2882, Suzorite 325-S" type="15" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.142799" analysis="12.160"/>
<oxide symbol="SiO2" formula="0.856813" analysis="42.990"/>
<oxide symbol="F" formula="0.285586" analysis="4.530"/>
<oxide symbol="K2O" formula="0.142798" analysis="11.230"/>
<oxide symbol="MgO" formula="0.857202" analysis="28.840"/>
</chemistry>
</material>
<material name="Talc" weight="126.45120803263" dfnumber="1620" searchkey="Magnesium Silicate, Steatite, French Chalk, Hydrated talc" type="15,17,20" property1="0">
<chemistry>
<oxide symbol="SiO2" formula="1.333524" analysis="63.380"/>
<oxide symbol="MgO" formula="1.000000" analysis="31.870"/>
</chemistry>
</material>
<material name="Tektamer 38 Biocide" weight="0" dfnumber="1628" searchkey="" type="2" property1="0"/>
<material name="Tennessee #1 SGP" weight="381.86708282835" dfnumber="1629" searchkey="SGP #1 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.095268" analysis="2.000"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="26.800"/>
<oxide symbol="CaO" formula="0.013569" analysis="0.200"/>
<oxide symbol="SiO2" formula="3.729977" analysis="58.900"/>
<oxide symbol="K2O" formula="0.024242" analysis="0.600"/>
<oxide symbol="Fe2O3" formula="0.026166" analysis="1.100"/>
<oxide symbol="MgO" formula="0.037776" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.012277" analysis="0.200"/>
</chemistry>
</material>
<material name="Tennessee #10 Ball Clay" weight="330.13455583351" dfnumber="1630" searchkey="TENN #10" type="7" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.021025" analysis="0.600"/>
<oxide symbol="Fe2O3" formula="0.020837" analysis="1.010"/>
<oxide symbol="MgO" formula="0.024573" analysis="0.300"/>
<oxide symbol="Na2O" formula="0.031945" analysis="0.600"/>
<oxide symbol="TiO2" formula="0.061971" analysis="1.500"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="30.900"/>
<oxide symbol="CaO" formula="0.023536" analysis="0.400"/>
<oxide symbol="SiO2" formula="2.900021" analysis="52.800"/>
</chemistry>
</material>
<material name="Tennessee #5 Ball" weight="365.59139784946" dfnumber="1631" searchkey="Tennessee No. 5" type="7" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="0.054907" analysis="1.200"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="27.900"/>
<oxide symbol="CaO" formula="0.019550" analysis="0.300"/>
<oxide symbol="SiO2" formula="3.357844" analysis="55.200"/>
<oxide symbol="K2O" formula="0.038810" analysis="1.000"/>
<oxide symbol="Fe2O3" formula="0.025134" analysis="1.100"/>
<oxide symbol="MgO" formula="0.036287" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.017690" analysis="0.300"/>
</chemistry>
</material>
<material name="TI-21 Ball Clay" weight="373.37477337477" dfnumber="1640" searchkey="Hick TI-21, Old Hickory TI-21 Ball Clay" type="7" property1="0">
<chemistry>
<oxide symbol="K2O" formula="0.001983" analysis="0.050"/>
<oxide symbol="Fe2O3" formula="0.023352" analysis="1.000"/>
<oxide symbol="MgO" formula="0.018542" analysis="0.200"/>
<oxide symbol="Na2O" formula="0.005424" analysis="0.090"/>
<oxide symbol="TiO2" formula="0.073884" analysis="1.580"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="27.300"/>
<oxide symbol="CaO" formula="0.004662" analysis="0.070"/>
<oxide symbol="SiO2" formula="3.652338" analysis="58.750"/>
</chemistry>
</material>
<material name="Tile #6 Kaolin" weight="267.09753766328" dfnumber="1641" searchkey="Tile 6, Tile#6 Kaolin" type="18" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.100"/>
<oxide symbol="SiO2" formula="2.026806" analysis="45.500"/>
<oxide symbol="CaO" formula="0.014316" analysis="0.300"/>
<oxide symbol="Fe2O3" formula="0.008366" analysis="0.500"/>
<oxide symbol="MgO" formula="0.026572" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.004318" analysis="0.100"/>
<oxide symbol="TiO2" formula="0.046909" analysis="1.400"/>
</chemistry>
</material>
<material name="Tin Oxide" weight="150.71" dfnumber="1642" searchkey="Stannic Oxide, Tin(IV) Oxide, Tin Dioxide, SnO2" type="17,23" property1="0">
<chemistry>
<oxide symbol="SnO2" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Titanium Dioxide" weight="79.9" dfnumber="1644" searchkey="TiO2" type="17,23" property1="0">
<chemistry>
<oxide symbol="TiO2" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Tricalcium Phosphate" weight="310.06514423077" dfnumber="1650" searchkey="Tri-Calcium Phos, Tribasic Calcium Phosphate, Synthetic Bone Ash, Calcium Orthophosphate" type="17,23" property1="0">
<chemistry>
<oxide symbol="CaO" formula="2.997596" analysis="54.230"/>
<oxide symbol="P2O5" formula="1.000000" analysis="45.760"/>
</chemistry>
</material>
<material name="Turkish Colemanite" weight="193.31949375093" dfnumber="2166" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="B2O3" formula="1.146880" analysis="41.400"/>
<oxide symbol="SrO" formula="0.013028" analysis="0.700"/>
<oxide symbol="Al2O3" formula="0.001890" analysis="0.100"/>
<oxide symbol="Na2O" formula="0.003110" analysis="0.100"/>
<oxide symbol="Fe2O3" formula="0.001205" analysis="0.100"/>
<oxide symbol="MgO" formula="0.086118" analysis="1.800"/>
<oxide symbol="SiO2" formula="0.160407" analysis="5.000"/>
<oxide symbol="CaO" formula="0.910772" analysis="26.500"/>
</chemistry>
</material>
<material name="Turkish Ulexite" weight="202.29204004628" dfnumber="1657" searchkey="" type="15" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.003967" analysis="0.200"/>
<oxide symbol="SiO2" formula="0.175028" analysis="5.200"/>
<oxide symbol="CaO" formula="0.710366" analysis="19.700"/>
<oxide symbol="MgO" formula="0.100393" analysis="2.000"/>
<oxide symbol="Na2O" formula="0.189241" analysis="5.800"/>
<oxide symbol="B2O3" formula="0.964956" analysis="33.200"/>
</chemistry>
</material>
<material name="Ulexite" weight="270.16304789174" dfnumber="1660" searchkey="Television Stone" type="15,17" property1="0">
<chemistry>
<oxide symbol="CaO" formula="0.666602" analysis="13.840"/>
<oxide symbol="Na2O" formula="0.333398" analysis="7.650"/>
<oxide symbol="B2O3" formula="1.667429" analysis="42.950"/>
</chemistry>
</material>
<material name="Ultrox" weight="189.56923076923" dfnumber="1665" searchkey="" type="23" property1="0">
<chemistry>
<oxide symbol="ZrO2" formula="1.000000" analysis="65.000"/>
<oxide symbol="SiO2" formula="1.103981" analysis="35.000"/>
</chemistry>
</material>
<material name="Unispar 50" weight="518.51799213916" dfnumber="2352" searchkey="Unispar-50" type="13" property1="0">
<chemistry>
<oxide symbol="Na2O" formula="0.577985" analysis="6.900"/>
<oxide symbol="K2O" formula="0.264636" analysis="4.800"/>
<oxide symbol="Al2O3" formula="0.997965" analysis="19.600"/>
<oxide symbol="SiO2" formula="5.772464" analysis="66.800"/>
<oxide symbol="Fe2O3" formula="0.001298" analysis="0.040"/>
<oxide symbol="CaO" formula="0.157378" analysis="1.700"/>
</chemistry>
</material>
<material name="VanTalc" weight="128.94709394347" dfnumber="3112" searchkey="" type="" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.012602" analysis="1.000"/>
<oxide symbol="SiO2" formula="1.304639" analysis="61.000"/>
<oxide symbol="Fe2O3" formula="0.010444" analysis="1.300"/>
<oxide symbol="MgO" formula="0.988762" analysis="31.000"/>
<oxide symbol="CaO" formula="0.009165" analysis="0.400"/>
<oxide symbol="Na2O" formula="0.002073" analysis="0.100"/>
</chemistry>
</material>
<material name="Veegum" weight="0" dfnumber="1672" searchkey="Veegum T, Veegum CER, Veegum Pro, VGT" type="2,8" property1="0"/>
<material name="Velvacast Kaolin" weight="262.17378369372" dfnumber="1673" searchkey="Velva Cast" type="18" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="38.910"/>
<oxide symbol="SiO2" formula="1.984177" analysis="45.490"/>
<oxide symbol="Fe2O3" formula="0.006062" analysis="0.370"/>
<oxide symbol="CaO" formula="0.012149" analysis="0.260"/>
<oxide symbol="MgO" formula="0.011709" analysis="0.180"/>
<oxide symbol="TiO2" formula="0.036090" analysis="1.100"/>
</chemistry>
</material>
<material name="Virginia Kyanite" weight="170.26672843734" dfnumber="2325" searchkey="" type="17" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.009685" analysis="0.910"/>
<oxide symbol="MgO" formula="0.002535" analysis="0.060"/>
<oxide symbol="SiO2" formula="1.061370" analysis="37.460"/>
<oxide symbol="K2O" formula="0.003615" analysis="0.200"/>
<oxide symbol="Na2O" formula="0.005493" analysis="0.200"/>
<oxide symbol="TiO2" formula="0.019607" analysis="0.920"/>
<oxide symbol="Al2O3" formula="1.000000" analysis="59.900"/>
<oxide symbol="CaO" formula="0.001518" analysis="0.050"/>
</chemistry>
</material>
<material name="vol353cer Hectorite" weight="145.34288936053" dfnumber="1682" searchkey="" type="9" property1="0">
<chemistry>
<oxide symbol="Fe2O3" formula="0.014089" analysis="1.550"/>
<oxide symbol="MgO" formula="0.685671" analysis="19.000"/>
<oxide symbol="Na2O" formula="0.055124" analysis="2.350"/>
<oxide symbol="TiO2" formula="0.004915" analysis="0.270"/>
<oxide symbol="CaO" formula="0.174729" analysis="6.740"/>
<oxide symbol="Al2O3" formula="0.054324" analysis="3.810"/>
<oxide symbol="K2O" formula="0.011270" analysis="0.730"/>
<oxide symbol="SiO2" formula="1.050226" analysis="43.400"/>
<oxide symbol="Li2O" formula="0.073205" analysis="1.500"/>
</chemistry>
</material>
<material name="Volcanic Ash" weight="387.85613343266" dfnumber="1689" searchkey="Pumicite" type="15,17" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.573272" analysis="15.000"/>
<oxide symbol="SiO2" formula="4.345802" analysis="67.000"/>
<oxide symbol="CaO" formula="0.416925" analysis="6.000"/>
<oxide symbol="Fe2O3" formula="0.048728" analysis="2.000"/>
<oxide symbol="K2O" formula="0.041383" analysis="1.000"/>
<oxide symbol="TiO2" formula="0.024395" analysis="0.500"/>
<oxide symbol="Na2O" formula="0.251500" analysis="4.000"/>
<oxide symbol="MgO" formula="0.290192" analysis="3.000"/>
</chemistry>
</material>
<material name="Wollastonite" weight="116.19718309859" dfnumber="1705" searchkey="Wolastonite" type="15,17" property1="0">
<chemistry>
<oxide symbol="CaO" formula="1.000000" analysis="48.280"/>
<oxide symbol="SiO2" formula="0.999953" analysis="51.720"/>
</chemistry>
</material>
<material name="Wollastonite Vansil" weight="126.87050003382" dfnumber="1706" searchkey="Vansil" type="15" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="0.022253" analysis="1.800"/>
<oxide symbol="CaO" formula="0.946295" analysis="42.100"/>
<oxide symbol="SiO2" formula="1.088930" analysis="51.900"/>
<oxide symbol="K2O" formula="0.000669" analysis="0.050"/>
<oxide symbol="Fe2O3" formula="0.006305" analysis="0.800"/>
<oxide symbol="MgO" formula="0.046935" analysis="1.500"/>
<oxide symbol="Na2O" formula="0.006102" analysis="0.300"/>
<oxide symbol="TiO2" formula="0.000789" analysis="0.050"/>
</chemistry>
</material>
<material name="Wood Ash" weight="0" dfnumber="2138" searchkey="" type="15" property1="0"/>
<material name="Yellow Ochre" weight="512.04819277108" dfnumber="1714" searchkey="Hydrated ferric oxide" type="9" property1="0">
<chemistry>
<oxide symbol="Al2O3" formula="1.000000" analysis="19.920"/>
<oxide symbol="SiO2" formula="4.922819" analysis="57.780"/>
<oxide symbol="Fe2O3" formula="0.704386" analysis="22.010"/>
<oxide symbol="CaO" formula="0.020993" analysis="0.230"/>
<oxide symbol="MgO" formula="0.007624" analysis="0.060"/>
</chemistry>
</material>
<material name="Zinc Oxide" weight="81.4" dfnumber="1718" searchkey="ZnO, Zincite" type="15,17" property1="0">
<chemistry>
<oxide symbol="ZnO" formula="1.000000" analysis="100.000"/>
</chemistry>
</material>
<material name="Zircopax" weight="183.33581312305" dfnumber="1724" searchkey="" type="23" property1="0">
<chemistry>
<oxide symbol="ZrO2" formula="1.000000" analysis="67.210"/>
<oxide symbol="SiO2" formula="1.000263" analysis="32.790"/>
</chemistry>
</material>
</materials>